Temperature stability of SmCo (2:17) magnets modified by Ni–Cr two‐layer coating
Source abstract
Abstract
Abstract The oxidation resistance behavior of SmCo (2:17)‐type high‐temperature magnets modified with Ni–Cr two‐layer coating was studied. The study depicts the mass gain kinetics and magnetic properties of uncoated and Ni–Cr‐modified magnets oxidized at high temperature (500 °C) in air for 200 h. The oxidation test results illustrate that the mass gain of uncoated magnet is 6.95 mg·cm −2 which is more than that (0.08 mg·cm −2 ) of coated magnet after 200 h. For the magnetic properties concerned, there is a great loss for uncoated magnet, while for coated magnet, magnetic properties do not change much. The study of uncoated magnet through X‐ray diffraction (XRD) and electron probe microanalysis (EPMA) shows that the invasion of oxygen at high temperature leads to the loss of magnetic properties by changing the microstructure of magnet.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Magnetic properties of thin films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering Beihang University 100191 Beijing China
National Center of Physics Quaid‐e‐Azam University 45320 Islamabad Pakistan
Funding
National Natural Science Foundation of China · Natural Science Foundation of Beijing Municipality · Natural Science Foundation of Beijing Municipality (CN)
References (31)
Show source-provided references
1. 10.1016/S0304‐8853(00)00508‐410.1016/S0304‐8853(00)00508‐4 ↗
2. Room‐and high‐temperature magnetic properties of Sm(CobalFe x Cu0.088Zr0.025)7.5 (x = 0–0.30) sintered magnets
3. RichardTF RubertusCS. Air force applications of advanced magnetic materials. In:Proceeding of Materials Research Society Spring Conference Vol 57. San Francisco;1999.481.
4. 10.1109/20.90880510.1109/20.908805 ↗
5. 10.1063/1.163914510.1063/1.1639145 ↗
6. Review of research on 2:17 type SmCo rare earth permanent magnets
7. 10.1007/s12598‐013‐0162‐610.1007/s12598‐013‐0162‐6 ↗
8. 10.1063/1.360232110.1063/1.3602321 ↗
9. 10.1016/j.jmmm.2012.02.12210.1016/j.jmmm.2012.02.122 ↗
10. 10.1016/j.jmmm.2006.01.10710.1016/j.jmmm.2006.01.107 ↗
11. 10.1063/1.36959710.1063/1.369597 ↗
12. 10.1109/20.90877310.1109/20.908773 ↗
13. 10.1109/20.95122510.1109/20.951225 ↗
14. 10.1063/1.491387610.1063/1.4913876 ↗
15. 10.1007/s10948‐011‐1276‐410.1007/s10948‐011‐1276‐4 ↗
16. 10.1179/mst.1989.5.8.78010.1179/mst.1989.5.8.780 ↗
17. 10.1109/TMAG.2004.82932310.1109/TMAG.2004.829323 ↗
18. 10.1016/j.surfcoat.2006.07.23310.1016/j.surfcoat.2006.07.233 ↗
19. 10.1016/j.jmmm.2012.11.01310.1016/j.jmmm.2012.11.013 ↗
20. 10.1016/j.jallcom.2011.12.03110.1016/j.jallcom.2011.12.031 ↗
21. 10.1016/j.jallcom.2009.07.11510.1016/j.jallcom.2009.07.115 ↗
22. 10.1016/j.corsci.2013.07.03310.1016/j.corsci.2013.07.033 ↗
23. 10.1063/1.356519610.1063/1.3565196 ↗
24. 10.1109/TED.2005.84586810.1109/TED.2005.845868 ↗
25. 10.1016/j.jmmm.2004.11.40810.1016/j.jmmm.2004.11.408 ↗
26. 10.1109/TMAG.2004.82919510.1109/TMAG.2004.829195 ↗
27. 10.1016/j.corsci.2012.04.02810.1016/j.corsci.2012.04.028 ↗
28. 10.1016/j.surfcoat.2013.03.03110.1016/j.surfcoat.2013.03.031 ↗
29. 10.1016/S1006‐706X(08)60168‐510.1016/S1006‐706X(08)60168‐5 ↗
30. 10.1016/S1001‐0521(07)60219‐810.1016/S1001‐0521(07)60219‐8 ↗
31. 10.1016/j.jmmm.2012.07.00610.1016/j.jmmm.2012.07.006 ↗