Sintering of WC-Co powder with nanocrystalline WC by spark plasma sintering
Source abstract
Abstract
A 92WC-8Co powder mixture with 33 nm WC grains was prepared by strengthening ball milling and was then sintered by spark plasma sintering (SPS) at 1000-1200°C for 5-18 min under 10-25 kN, respectively. Movement of the position of low punch shown shrinkage of the sintered body began above 800°C. The shrinkage slowly rose as the temperature rose from 800 to 1000°C and then quickly rose at above 1000°C and then gradually rose at above 1150°C. The densities of the samples increased with an increase in sintering temperature, rapidly below 1100°C, and then gradually above 1100°C. WC grains grow gradually with increasing sintering temperature. The powder was sintered to near full density at 1100°C for 5 min under 10 kN. The best result of the sample with 275 nm WC grains and no pores was obtained at 1150°C under 10 kN for 5 min. The research found the graphite die had a function of carburization, which could compensate the sintered body for the lack of carbon, and had the normal microstructure.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Powder Metallurgy Techniques and Materials · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.