Microstructure and tensile properties of low cost titanium alloys at different cooling rate
Source abstract
Abstract
Abstract Titanium and titanium alloys have several advantages, but the cost of titanium alloys is very expensive compared with the traditional metal materials. This article introduces two new low‐cost titanium alloys Ti‐2.1Cr‐1.3Fe (TCF alloy) and Ti‐3Al‐2.1Cr‐1.3Fe (TACF alloy). In this study, we used Cr‐Fe master alloy as one of the raw materials to develop the two new alloys. We introduce the microstructure and tensile properties of the two new alloys from β solution treated with different cooling methods. Optical microscopy (OM), X‐ray diffractometry (XRD), and transmission electron microscopy (TEM) were employed to analyze the phase constitution, and scanning electron microscopy (SEM) was used to observe the fracture surfaces. The results indicate that the microstructures consist of β grain boundary and α′ martensite after water quenching (WQ), β matrix and α phase after air cooling (AC) and furnace cooling (FC), respectively. Also, the microstructure is the typical basketweave structures after FC. Of course, athermal ω is also observed by TEM after WQ. The strength increases with decreasing cooling rates and the plasticity is reversed. Because of the athermal ω, the strength and ductility are highest and lowest when the cooling method is WQ. The strength of TACF alloy is higher than the TCF alloy, but the plasticity is lower. The fracture surfaces are almost entirely covered with dimples under the cooling methods of AC and FC. Also, we observe an intergranular fracture area that is generated by athermal ω, although some dimples are observed after WQ.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory for Fabrication & Processing of Nonferrous Metals General Research Institute for Nonferrous Metals 100088 Beijing China
References (20)
Show source-provided references
1. 10.1007/s12598‐011‐0429‐810.1007/s12598‐011‐0429‐8 ↗
2. 10.1007/s12598‐010‐0179‐z10.1007/s12598‐010‐0179‐z ↗
3. 10.1007/s12598‐009‐0068‐510.1007/s12598‐009‐0068‐5 ↗
4. Application of Titanium and its alloys for automobile parts
5. 10.1007/s11837‐998‐0408‐110.1007/s11837‐998‐0408‐1 ↗
6. 10.1007/s11837‐001‐0143‐310.1007/s11837‐001‐0143‐3 ↗
7. 10.1016/S0026‐0657(09)70040‐210.1016/S0026‐0657(09)70040‐2 ↗
8. KawabeY. Research activities on cost effective metallurgy of titanium alloys in Japan [in]Proc. of 9th World Conference on Titanium Russia 1999:1275.
9. Development and applications of low cost titanium alloys
10. 10.1016/j.msea.2006.10.16610.1016/j.msea.2006.10.166 ↗
11. 10.1016/0921-5093(96)10245-810.1016/0921-5093(96)10245-8 ↗
12. 10.2464/jilm.55.54910.2464/jilm.55.549 ↗
13. Research on low cost titanium alloys
14. 10.2320/matertrans.46.157010.2320/matertrans.46.1570 ↗
15. 10.1016/j.msec.2004.12.01510.1016/j.msec.2004.12.015 ↗
16. Influence of cooling rate on microstructure and mechanical properties of beta processed TC11 alloy
17. 10.2320/matertrans.45.156610.2320/matertrans.45.1566 ↗
18. Mechanism of V and Cr on mechanical properties of Ti40 burn resistant titanium alloy
19. 10.1016/j.msea.2010.07.05510.1016/j.msea.2010.07.055 ↗
20. Effects of Al and Mo on mechanical properties of cast titanium alloys