Microstructural evolution, tensile property and dynamic compressive property of FSWed Ti–6Al–4V alloy
Source abstract
Abstract
Abstract Friction stir welding was applied to Ti–6Al–4V plates with 5 mm in thickness. The microstructure and mechanical properties were investigated. A full lamellar microstructure was developed near the top surface, and the size of prior β grain gradually decreases as the distance from the top surface increases. The microstructure of the bottom is fine equiaxed α grains, and the mean size is 2 μm. A mixture microstructure consisting of primary α, lamellar α + β and fine equiaxed α is discovered in thermomechanically affected zone (TMAZ). Results of transverse tensile test show that the tensile strength of the joint reaches 98% that of the base material (BM). Quasi‐static compression test shows that the joint exhibits larger compressive strength and failure strain than the BM. Dynamic compressive strength of the joint is close to that of the BM; furthermore, the strain at the peak stress and energy absorption of the joint are larger than those of the BM.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering Beijing Institute of Technology 100081 Beijing China
Funding
National Natural Science Foundation of China
References (33)
Show source-provided references
1. 10.1016/j.mser.2005.07.00110.1016/j.mser.2005.07.001 ↗
2. 10.1007/s12598‐016‐0704‐910.1007/s12598‐016‐0704‐9 ↗
3. 10.1007/s11661‐010‐0434‐910.1007/s11661‐010‐0434‐9 ↗
4. 10.1007/s11661‐010‐0439‐410.1007/s11661‐010‐0439‐4 ↗
5. 10.1016/j.matdes.2012.12.02410.1016/j.matdes.2012.12.024 ↗
6. 10.1016/j.msea.2010.02.02310.1016/j.msea.2010.02.023 ↗
7. 10.1016/j.matdes.2012.10.05110.1016/j.matdes.2012.10.051 ↗
8. 10.1179/1362171815Y.000000004310.1179/1362171815Y.0000000043 ↗
9. 10.1016/j.matdes.2015.09.12810.1016/j.matdes.2015.09.128 ↗
10. 10.1016/j.matchar.2015.06.02510.1016/j.matchar.2015.06.025 ↗
11. 10.1016/j.jmatprotec.2015.09.04110.1016/j.jmatprotec.2015.09.041 ↗
12. 10.1016/j.msea.2013.02.02510.1016/j.msea.2013.02.025 ↗
13. 10.1007/s11665‐014‐1075‐810.1007/s11665‐014‐1075‐8 ↗
14. 10.1016/j.msea.2007.08.05110.1016/j.msea.2007.08.051 ↗
15. Microstructure and properties of bonding interface in explosive welded AZ31/1060 composite plate
16. 10.1016/j.ijfatigue.2014.09.01310.1016/j.ijfatigue.2014.09.013 ↗
17. 10.1016/j.ijfatigue.2015.01.01210.1016/j.ijfatigue.2015.01.012 ↗
18. 10.1115/1.400130210.1115/1.4001302 ↗
19. 10.1179/136217110X1266577834842510.1179/136217110X12665778348425 ↗
20. 10.1007/s11665‐015‐1610‐210.1007/s11665‐015‐1610‐2 ↗
21. 10.1179/136217109X42583810.1179/136217109X425838 ↗
22. 10.1016/j.jmatprotec.2014.11.04610.1016/j.jmatprotec.2014.11.046 ↗
23. 10.1016/j.matdes.2010.01.02310.1016/j.matdes.2010.01.023 ↗
24. 10.1007/s11837‐015‐1376‐x10.1007/s11837‐015‐1376‐x ↗
25. 10.1016/j.scriptamat.2005.09.00810.1016/j.scriptamat.2005.09.008 ↗
26. 10.1016/j.msea.2009.07.01710.1016/j.msea.2009.07.017 ↗
27. 10.1016/j.scriptamat.2005.10.06210.1016/j.scriptamat.2005.10.062 ↗
28. 10.1007/s10853‐009‐3881‐110.1007/s10853‐009‐3881‐1 ↗
29. 10.1016/j.scriptamat.2009.08.01210.1016/j.scriptamat.2009.08.012 ↗
30. 10.1016/j.matdes.2009.12.01410.1016/j.matdes.2009.12.014 ↗
31. 10.1016/j.matdes.2009.08.02510.1016/j.matdes.2009.08.025 ↗
32. 10.1016/j.scriptamat.2014.01.01710.1016/j.scriptamat.2014.01.017 ↗
33. 10.1016/S1003‐6326(09)60388‐510.1016/S1003‐6326(09)60388‐5 ↗