Abstract

Abstract Effects of surface condition on fatigue properties of a medium‐strength γ ‐ TiAl alloy Ti–45Al–5Nb–1W (at%) were investigated. It is found that the maximum stresses of fatigue samples are lower than the yield stresses of the medium‐strength γ ‐ TiAl alloy. Meanwhile, the local plastic deformation is unconspicuous to occur at the crack tip. In this case, the fatigue strength is mainly decided by surface conditions of maximum‐stressed surface, but compressive stress and deformation especially resulted from shot peening play an important role in the improvement of the condition fatigue strength. The affecting depth of shot peening is about 250 μm. As a result, the relatively weak microstructures and phases become the preferential initiation sites and propagation routes. They are observed to be equiaxed γ grains, B2 + ω grains, and α 2 ‐γ lamellar interface in soft orientations. The existence of V‐notch can significantly reduce the fatigue properties of the samples.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Energetic Materials and Combustion · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Key Laboratory of Advanced Technologies of Materials, Ministry of Education School of Materials Science and Engineering Southwest Jiaotong University 610031 Chengdu China

Funding

National Natural Science Foundation of China · the National Natural Science Foundation of China · the National Higher-education Institution General Research and Development Funding

References (20)

Show source-provided references
1. 10.1016/S0921‐5093(98)01158‐710.1016/S0921‐5093(98)01158‐7 ↗
2. Effect of silver addition in gamma titanium aluminide
3. 10.1016/j.matdes.2009.10.04510.1016/j.matdes.2009.10.045 ↗
4. 10.1016/j.intermet.2009.07.00710.1016/j.intermet.2009.07.007 ↗
5. Cyclic crack growth in titanium aluminides
6. 10.1016/j.actamat.2004.11.02210.1016/j.actamat.2004.11.022 ↗
7. 10.1016/S1359‐6454(01)00092‐110.1016/S1359‐6454(01)00092‐1 ↗
8. 10.1016/S1359‐6454(01)00091‐X10.1016/S1359‐6454(01)00091‐X ↗
9. 10.1016/j.intermet.2004.09.00710.1016/j.intermet.2004.09.007 ↗
10. The effect of machined topography and integrity on fatigue life
11. Microstructure and mechanical properties of a forged β‐solidifying γ TiAl alloy in different heat treatment conditions
12. 10.1046/j.1460‐2695.2002.00549.x10.1046/j.1460‐2695.2002.00549.x ↗
13. 10.1016/j.actamat.2007.12.01310.1016/j.actamat.2007.12.013 ↗
14. Effects of stress concentrations on the fatigue life of a gamma‐based titanium aluminide
15. 10.1016/0013‐7944(94)90149‐X10.1016/0013‐7944(94)90149‐X ↗
16. 10.1007/BF0003468710.1007/BF00034687 ↗
17. 10.1016/j.msea.2014.07.06310.1016/j.msea.2014.07.063 ↗
18. An approach for prediction of fatigue strength of shot peened components
19. 10.1007/s12598‐014‐0238‐y10.1007/s12598‐014‐0238‐y ↗
20. Effects of varied surface condition on the fatigue behavior of a high‐strength gamma‐based titanium aluminide alloy