Interface reactions between TiAl alloys and diacetatozirconic acid–yttria molds differentiated by ammonium metatungstate addition
Source abstract
Abstract
Abstract Two types of diacetatozirconic acid–yttria molds which were labeled as ZYW mold (diacetatozirconic acid–yttria mold with traces of ammonium metatungstate in the slurry) and ZY mold (diacetatozirconic acid–yttria mold without ammonium metatungstate) were prepared by traditional investment casting. The ZYW and ZY molds were sintered in a carbon‐reducing atmosphere and in air, respectively, at 1550 °C for 4 h. Interactions between Ti–47Al–2Cr–2Nb (at%) alloys and the molds at 1650 °C for 30 min were studied. The microstructures of the metal–mold interfaces and the presence of inclusions and oxygen contamination in the TiAl bulk alloy were analyzed, and the influences of ammonium metatungstate were discussed. The results indicate that WO 3 releases O into the TiAl melt, introducing tungsten metal into the alloy matrix. The TiAl alloy ingots cast in the ZY molds had the fewest inclusions and the lowest oxygen contamination.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
College of Materials Science and Engineering Beijing University of Technology 100124 Beijing China
Beijing Institute of Astronautical Systems Engineering 100076 Beijing China
Funding
National Natural Science Foundation of China · Natural Science Foundation of Beijing Municipality
References (19)
Show source-provided references
1. 10.1016/j.intermet.2004.12.02110.1016/j.intermet.2004.12.021 ↗
2. 10.1016/j.paerosci.2012.04.00110.1016/j.paerosci.2012.04.001 ↗
3. Recent developments in the induction skull melting and investment casting of titanium aluminides
4. 10.1515/htmp-2012-012010.1515/htmp-2012-0120 ↗
5. 10.1016/S0921-5093(97)00632-110.1016/S0921-5093(97)00632-1 ↗
6. 10.1016/S0921-5093(01)01494-010.1016/S0921-5093(01)01494-0 ↗
7. 10.1016/j.intermet.2004.12.00610.1016/j.intermet.2004.12.006 ↗
8. 10.1016/j.intermet.2010.11.00710.1016/j.intermet.2010.11.007 ↗
9. 10.1016/j.jeurceramsoc.2012.11.00610.1016/j.jeurceramsoc.2012.11.006 ↗
10. 10.1016/j.intermet.2007.08.00710.1016/j.intermet.2007.08.007 ↗
11. 10.1016/S0921-5093(01)01584-210.1016/S0921-5093(01)01584-2 ↗
12. 10.1016/j.jmatprotec.2010.03.00310.1016/j.jmatprotec.2010.03.003 ↗
13. 10.1016/j.intermet.2010.11.02210.1016/j.intermet.2010.11.022 ↗
14. 10.1016/S1875-5372(13)60091-010.1016/S1875-5372(13)60091-0 ↗
15. Centrifugal casting of large thin‐wall cylindrical structure of titanium alloys
16. MattsonRK PaulinyTA TeramuraT Facecoat ceramic slurry and methods for use thereof in mold fabrication and casting. US Patent; 5827791.1998.
17. Method of preparing titanium alloy investment casting binder—diacetatozirconic acid
18. Interaction between TiAl alloy and diacetatozirconic acid‐bonded yttria mould under high‐temperature and long‐term
19. 10.1016/S0925-8388(01)02028-X10.1016/S0925-8388(01)02028-X ↗