Abstract
Abstract In this paper, the AlMgB 14 and AlMgB 14 –TiB 2 composites were synthesized by means of mechanical alloying and the field‐activated and pressure‐assisted synthesis process. The effect of temperature and pressure on the purity and property of products was discussed. The results show that the process of preparing AlMgB 14 bulk materials is optimized as follows: synthesis temperature 1,400–1,500 °C, heating rate 100 °C·min −1 , axial pressure 60 MPa, heat preservation 8–10 min, optimum starting powders’ ratio Al: Mg: B = 0.1915:0.1363:0.6722, and adding excessive 3 wt% Al. The abrasion resistance of AlMgB 14 composites with varying amounts of TiB 2 was studied using single‐point diamond scratch tests with loads ranging from 10 to 100 N in 10 N increments. The scratch width increases almost linearly with the applied load and decreases with TiB 2 proportion increasing up to 70 wt%. With its advantages of fast heating, short reaction time, energy conservation, and high purity, this method offers a new way to synthesize AlMgB 14 and AlMgB 14 –TiB 2 composites.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Boron and Carbon Nanomaterials Research · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
College of Materials Science and Engineering Taiyuan University of Technology 030024 Taiyuan China
College of Mechanical and Electrical Engineering Qingdao Binhai University 266555 Qingdao China
Institute of Chemical and Biological Technology Taiyuan University of Science and Technology 030021 Taiyuan China
Funding
National Natural Science Foundation of China
References (20)
Show source-provided references
1. 10.1016/S1359‐6462(99)00400‐510.1016/S1359‐6462(99)00400‐5 ↗
2. 10.1016/j.jallcom.2003.07.00710.1016/j.jallcom.2003.07.007 ↗
3. 10.1016/j.ijrmhm.2008.07.00910.1016/j.ijrmhm.2008.07.009 ↗
4. 10.1016/j.jallcom.2007.01.18710.1016/j.jallcom.2007.01.187 ↗
5. 10.1016/S0022‐0248(07)80108‐410.1016/S0022‐0248(07)80108‐4 ↗
6. 10.1016/j.jssc.2003.02.00510.1016/j.jssc.2003.02.005 ↗
7. 10.1016/j.ijrmhm.2008.07.00910.1016/j.ijrmhm.2008.07.009 ↗
8. 10.1016/j.jallcom.2011.05.03310.1016/j.jallcom.2011.05.033 ↗
9. 10.1016/S0921‐5093(00)00765‐610.1016/S0921‐5093(00)00765‐6 ↗
10. 10.1016/j.msea.2003.10.27110.1016/j.msea.2003.10.271 ↗
11. In‐situ synthesis of (TiC)_pNi/TiAl/Ti functional gradient materials via field‐activated process
12. 10.1016/j.msea.2012.01.02010.1016/j.msea.2012.01.020 ↗
13. 10.1088/1674‐1056/21/1/01420210.1088/1674‐1056/21/1/014202 ↗
14. 10.1007/s11433‐012‐4657‐110.1007/s11433‐012‐4657‐1 ↗
15. 10.1007/s11433‐012‐4716‐710.1007/s11433‐012‐4716‐7 ↗
16. 10.1007/s12598‐012‐0490‐y10.1007/s12598‐012‐0490‐y ↗
17. 10.1080/0010220750894667110.1080/00102207508946671 ↗
18. 10.1016/j.jeurceramsoc.2006.04.11410.1016/j.jeurceramsoc.2006.04.114 ↗
19. 10.1007/s12598‐012‐0554‐z10.1007/s12598‐012‐0554‐z ↗
20. 10.1016/S0921‐5093(02)00835‐310.1016/S0921‐5093(02)00835‐3 ↗