Slag – Refractory Interactions During Ilmenite Smelting: Thermodynamic Simulation and Experimental Data
Source abstract
Abstract
The interaction of four types of commonly used refractories (i.e., burned magnesite brick, magnesia carbon brick, corundum castable, and SiC castable) with slag formed in the smelting of titanium (wt. [TiO2] = 80%) in an electric furnace at the Panzhihuan Iron and Steel plant was studied. Erosion of refractories by titanium slag was calculated using the FactSage software program. The experiment was carried out in an electric furnace based on calculation results. Meanwhile, the results of the thermodynamic simulation showed that the interaction of SiC castable with titanium slag formed TiC with a high melting point, which can prevent the slag from penetrating more deeply into the refractory and exhibits good erosion resistance. In terms of erosion resistance to titanium slag, different refractory materials can be arranged in order from most to least erosion resistant as follows: SiC castable → magnesia carbon brick → magnesite brick → corundum castable. The results of theoretical calculations are in good agreement with the experiment results.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Iron and Steelmaking Processes · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. H. G. Du, G. T. Xu, and R. S. Diao, “Microstructure analysis of iron corrosion lining of titanium bearing blast furnace slag,” Iron Steel Vanadium Titanium, 6(2) (2002).
2. H. G. Du, et al., “Study on erosion of blast furnace slag by blast furnace slag,” Iron Steel, 4(1), 56 – 59 (2003).
3. J. Li, “Study on the mechanism of slag corrosion and improvement of material properties of blast furnace in Panzhihua Iron & Steel Co.” (2002).
4. Q.-C. Liu, et al., “Corrosion resistance of MgO – C refractory to smelting reduction slag containing titania,” British Corrosion Journal, 37(3), 231 – 234 (2002).10.1179/000705902225004392 ↗
5. J. Qin, et al., “Melting reduction furnace lining erosion cause analysis and improvement measures,” Refractory Material, 4, No. 2, 152 – 154 (2013).
6. A. M. Garbers-Craig and P. C. Pistorius, “Slag-refractory interactions during the smelting of ilmenite,” South African Journal of Science, 102(11/12), 575 – 581 (2006).
7. S. B. Sang, et al., “Discussion on the furnace lining material of high titanium pellet melting furnace,” Silicate Bulletin, 6(4) (2014).
8. Y. Chen, G. A. Brooks, and S. A. Nightingale, “Slag line dissolution of MgO refractory,” Canadian Metallurgical Quarterly, 8(3), 323 – 330 (2005).10.1179/cmq.2005.44.3.323 ↗
9. W. Hu, et al., “Different matrix combined with the research on corrosion resistance of MgO–C brick for slag,” Silicate Bulletin, 6(1) (2011).
10. X. L. Fan, et al., “Slag resistance of MgO–C brick with different carbon content,” Journal of Wuhan University of Science and Technology, 5(4), 394 – 398 (2009).
11. H. C. Li, et al., “Effect of electromagnetic field on corrosion resistance of MgO–C refractories,” Journal of Silicate, 6(3), 452 – 457 (2011).
12. V. Muñoz, S. Camelli, and A. G. T. Martinez, “Slag corrosion of alumina-magnesiacarbon refractory bricks: experimental data and thermodynamic simulation,” Ceram. Int., 43(5), 4562 – 4569 (2017).10.1016/j.ceramint.2016.12.114 ↗
13. Z. Y. Chen, “Analysis of the corrosion of MgO–CaO materials by the phase diagram,” J. Metals, 8(2), 62 – 69 (1983).
14. J. Berjonneau, P. Prigent, and J. Poirier, “The development of a thermodynamic model for Al2O3–MgO refractory castable corrosion by secondary metallurgy steel ladle slags,” Ceram. Int., 35(2), 623 – 635 (2009).10.1016/j.ceramint.2008.04.002 ↗