High-cycle fatigue properties were investigated at 4, 77 and 293 K in Ti–5% Al–2.5% Sn ELI alloys, in which mean alpha grain sizes were about 30 mm in the rolled material and 80 mm in the forged material. The ultimate tensile strengths of both materials were almost same and increased with decreasing temperature. The fatigue strength of each material also tended to increase with decreasing temperature. At 293 K, the fatigue strength of each material was almost equivalent. At 4 and 77 K, however, the fatigue strength of the rolled material was higher than that of the forged material. Concerning the rolled material, the fatigue strengths at 106 cycles at 4 and 77 K were about 1.6 and 1.5 times higher than that at 293 K, respectively. On the other hand, in the forged material, it should be noted that the fatigue strengths in longer-life region (over 106 cycles) were almost equivalent not depending on test temperatures. Fatigue cracks initiated in the specimen interior independently of test temperatures and materials (we call this type of crack initiation ‘sub-surface crack initiation’) and formed facet-like structures at the sub-surface crack initiation sites at 4 and 77 K. The size of each facet-like structure corresponded closely to the grain size itself. The sizes of crack initiation sites were smaller in the rolled material than in the forged material. Since sub-surface cracks, which form facets or crack initiation sites, are supposed to act as defects, it is concluded that grain refinement leads to reduce the size of crack initiation site and this contributes effectively to improve the fatigue strength in high-cycle region at cryogenic temperatures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fatigue and fracture mechanics · Aluminum Alloy Microstructure Properties · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. T. Ogata · Proceedings of 23rd International Symposium on Space Technology and Science. Japan · 2002
2. Y. Tachi · Collected Abstracts of the 2002 Spring Meeting of the Japan, Institute of Metals · 2002
3. T. Yuri · J. Jpn Inst. Metals · 2002 · 66 · 128710.2320/jinstmet1952.66.12_1287 ↗
4. S. Matsuoka · 2002
5. H. Sumiyoshi · 2002
6. K. Nagai . · Trans. Iron Steel Inst. Jpn · 1987 · 27 · 37610.2355/isijinternational1966.27.376 ↗
7. 10.1016/0921-5093(90)90268-810.1016/0921-5093(90)90268-8 ↗
8. 10.1016/0036-9748(83)90385-X10.1016/0036-9748(83)90385-X ↗
9. 10.1016/0001-6160(76)90147-410.1016/0001-6160(76)90147-4 ↗
10. J. Rupppen · 1978 · 47
11. S. Adachi · 1985 · 2139
12. 10.1016/0921-5093(94)91005-710.1016/0921-5093(94)91005-7 ↗
13. 10.2355/isijinternational.37.117010.2355/isijinternational.37.1170 ↗
14. 10.1016/S0142-1123(98)00028-010.1016/S0142-1123(98)00028-0 ↗
15. 10.1046/j.1460-2695.1999.00187.x10.1046/j.1460-2695.1999.00187.x ↗
16. 10.1046/j.1460-2695.1999.00206.x10.1046/j.1460-2695.1999.00206.x ↗
17. T. Abe · J. Jpn Mech. · 2001 · 2001 · 1988
18. 10.1016/S1359-6462(01)01213-110.1016/S1359-6462(01)01213-1 ↗
19. 10.1046/j.1460-2695.2001.00459.x10.1046/j.1460-2695.2001.00459.x ↗
20. Y. Murakami · 2002
21. S. Nishijima · Material Strength Data Sheet Technical Document No.5 · 1989
22. K. Kanazawa · Material Strength Data Sheet Technical Document No.9 · 1995
23. S. Matsuoka · Material Strength Data Sheet Technical Document No.17 · 1997
24. 10.1007/BF0264404610.1007/BF02644046 ↗
25. S. Taira · 1978 · 135