journal article·2016-04

Fatigue behaviour of Al/steel dissimilar resistance spot welds fabricated using Al–Mg interlayer

I. Ibrahim, R. Ito, T. Kakiuchi, Y. Uematsu, K. Yun, C. Matsuda

Publisher page

Abstract

Aluminium alloy sheets were joined to stainless steel ones by a resistance spot welding method using Al–Mg alloy interlayer. The interlayer exhibits a lower melting point than the Al alloy. Consequently, melted interlayer with a lower temperature filled the gap between the two sheets and resulted in effective joining. Subsequently, tensile shear fatigue tests had been conducted to evaluate fatigue strength and to determine the fatigue fracture mechanism. Resistance spot welding dissimilar welds exhibited higher fatigue strengths than friction stir spot welded dissimilar ones. Fatigue fracture modes were dependent on the load levels, where plug type fracture occurred at high load levels, shear fracture through the nugget at medium load levels and through thickness fatigue crack propagation in the Al sheet at low load levels. The fracture mode transition was attributed to the geometrical rotation around the nugget.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Metal Forming Simulation Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Mechatronic Engineering, Universiti Malaysia Perlis, Arau, Perlis, 02600, Malaysia

Graduate School of Engineering, Gifu University, 1-1 Yanagido, Gifu, 501-1193, Japan

Department of Mechanical Engineering, Gifu University, Yanagido, Gifu, 501-1193, Japan

Department of Electrical, Electronic and Computer Engineering, Gifu University, 1-1 Yanagido, Gifu, 501-1193, Japan

References (21)

Show source-provided references
1. 10.1179/136217109X45696010.1179/136217109X456960 ↗
2. 10.1179/136217109X40043910.1179/136217109X400439 ↗
3. 10.1179/136217110X1278588954946210.1179/136217110X12785889549462 ↗
4. 10.1016/j.msea.2010.03.09710.1016/j.msea.2010.03.097 ↗
5. 10.1111/j.1460-2695.2010.01549.x10.1111/j.1460-2695.2010.01549.x ↗
6. 10.1179/1362171812Y.000000001410.1179/1362171812Y.0000000014 ↗
7. 10.2207/qjjws.14.31410.2207/qjjws.14.314 ↗
8. 10.1179/13621719910153760810.1179/136217199101537608 ↗
9. 10.1533/wint.2006.367710.1533/wint.2006.3677 ↗
10. 10.1016/j.matchar.2008.07.00510.1016/j.matchar.2008.07.005 ↗
11. 10.1016/j.jmatprotec.2008.11.00310.1016/j.jmatprotec.2008.11.003 ↗
12. 10.1016/j.matchar.2010.03.01510.1016/j.matchar.2010.03.015 ↗
13. 10.1016/S1359-6454(97)00318-210.1016/S1359-6454(97)00318-2 ↗
14. 10.1179/1362171810Y.000000000910.1179/1362171810Y.0000000009 ↗
15. 10.1016/j.msea.2011.12.09610.1016/j.msea.2011.12.096 ↗
16. 10.1179/1362171813Y.000000012910.1179/1362171813Y.0000000129 ↗
17. 10.1179/1362171815Y.000000002810.1179/1362171815Y.0000000028 ↗
18. Matsuda C. · Int. J. Metall. Mater. Sci. Eng · 2015 · 5 · 1
19. Matsuda C. · Proc. 8th · 53
20. 10.1179/136217108X33890810.1179/136217108X338908 ↗
21. Bulletin of Alloy Phase Diagrams, 1982, 3, (1), 60–74, Berlin, Springer.