journal article·2014-07

Similar and dissimilar resistance spot welding of advanced high strength steels: welding and heat treatment procedures, structure and mechanical properties

S. T. Wei, D. Lv, R. D. Liu, L. Lin, R. J. Xu, J. Y. Guo, K. Q. Wang

Publisher page

Abstract

Similar and dissimilar combinations of a 1000 MPa galvanised dual phase (DP) steel and a 980 MPa transformation induced plasticity (TRIP) steel were resistance spot welded under different welding and heat treatment parameters. The microstructure and mechanical properties of spot welds were evaluated using metallographic technique, microhardness and tensile shear tests. The results showed that the tendency to fail in the pullout mode increased in the order of DP/DP, TRIP/TRIP and DP/TRIP welds, which was caused by the different hardness distribution, carbon equivalent and susceptibility to shrinkage void formation of spot welds for different combinations. In the study of the effects of heat treatments on the DP/TRIP welds, the pre-heating procedure improved the splash of welding to some extent. When the cooling time was larger than or equal to 1000 ms, the post-heating procedure improved the mechanical properties of spot welds owing to the temper of spot weld microstructure.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Automobile and Home Appliance Steel Institute, Technology Center of Angang Steel Company Limited, 63 Wuyi Road, Anshan 114009, China

References (28)

Show source-provided references
1. de Cooman BC, Speer JG, Pyshmintsev IY, and Yoshinaga N: ‘Materials design: the key to modern steel products’, 1st edn, Chap. 7, ‘Low carbon steels’, 381–404; 2007, Bad Harzburg, GRIPS Media GmbH.
2. 10.1179/1362171813Y.000000012010.1179/1362171813Y.0000000120 ↗
3. 10.1080/0950711080241300110.1080/09507110802413001 ↗
4. Tumuluru MD · Weld. J. · 2006 · 85 · 31
5. 10.1016/j.jmatprotec.2008.05.03010.1016/j.jmatprotec.2008.05.030 ↗
6. 10.1016/j.jmatprotec.2008.06.00810.1016/j.jmatprotec.2008.06.008 ↗
7. 10.1016/j.actamat.2008.04.03510.1016/j.actamat.2008.04.035 ↗
8. 10.1179/174329308X32631810.1179/174329308X326318 ↗
9. 10.1179/174329308X27173310.1179/174329308X271733 ↗
10. Tumuluru M · Weld. J. · 2007 · 86 · 161s
11. 10.1179/136217110X1281339316973210.1179/136217110X12813393169732 ↗
12. Lane CT · Weld. J. · 1987 · 66 · 260s
13. Chuko WL · Weld. J. · 2002 · 81 · 1s
14. Khan MI, Kuntz ML, Zhou Y, Chan K, and Scotchmer N: ‘Monitoring the effect of RSW pulsing on AHSS using FEA (SORPAS) software’, SAE technical paper no. 2007-01-1370, SAE, Warrendale, PA, USA, 2007.10.4271/2007-01-1370 ↗
15. 10.1179/1362171811Y.000000005310.1179/1362171811Y.0000000053 ↗
16. 10.1179/1362171812Y.000000000610.1179/1362171812Y.0000000006 ↗
17. 10.1179/136217108X32547010.1179/136217108X325470 ↗
18. 10.1016/j.matdes.2006.10.01910.1016/j.matdes.2006.10.019 ↗
19. 10.1016/j.msea.2007.07.00710.1016/j.msea.2007.07.007 ↗
20. 10.1016/j.matdes.2010.09.01010.1016/j.matdes.2010.09.010 ↗
21. 10.1016/j.jmatprotec.2008.11.01710.1016/j.jmatprotec.2008.11.017 ↗
22. Marya M · Weld. J. · 2005 · 84 · 172s
23. 10.1016/j.msea.2010.07.09110.1016/j.msea.2010.07.091 ↗
24. Gould JE · Weld. J. · 2006 · 85 · 111s
25. 10.1016/B978-075068084-4/50009-110.1016/B978-075068084-4/50009-1 ↗
26. 10.1179/174329307X16440910.1179/174329307X164409 ↗
27. 10.1016/j.matdes.2008.09.03110.1016/j.matdes.2008.09.031 ↗
28. 10.1179/136217110X1281339316953410.1179/136217110X12813393169534 ↗