journal article·2021-08

Realising equal-strength welding with good conductivity in Cu–Cr–Zr alloy via friction stir welding

Y.D. Wang, S.Z. Zhu, G.M. Xie, L.H. Wu, P. Xue, D.R. Ni, B.L. Xiao, Z.Y. Ma

Publisher page

Abstract

Realising high-quality welding of the peak aged Cu–Cr–Zr alloy has always been a big challenge. Under a low rotation rate of 400 rev min −1 , equiaxed ultrafine grains together with nanoscale precipitates with comparable size to that of the peak aged state were obtained in the nugget zone of the friction stir welded joint. Further, the initial strengthened precipitates were also preserved near the nugget zone, neither dissolved nor coarsened. Therefore, softening zone disappeared and a high-quality weld with equal strength to the base material was first achieved. Furthermore, the electrical conductivity of the joint was hardly weakened. This study provides an effective method to improve the strength and electrical conductivity of the precipitation-hardened Cu alloy joints.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, University of Science and Technology of China, Shenyang, People's Republic of China

Shi-changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, People's Republic of China

State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang, People's Republic of China

Funding

National Natural Science Foundation of China · Open Research Fund from the State Key Laboratory of Rolling and Automation

References (30)

Show source-provided references
1. 10.1016/j.jallcom.2017.11.30910.1016/j.jallcom.2017.11.309 ↗
2. 10.1016/j.jnucmat.2018.07.05510.1016/j.jnucmat.2018.07.055 ↗
3. 10.1088/2053-1591/aaabc510.1088/2053-1591/aaabc5 ↗
4. 10.1016/j.jallcom.2018.09.04010.1016/j.jallcom.2018.09.040 ↗
5. 10.1016/j.jnucmat.2007.03.22010.1016/j.jnucmat.2007.03.220 ↗
6. 10.1016/j.jmst.2014.03.02510.1016/j.jmst.2014.03.025 ↗
7. 10.1007/s11665-015-1790-910.1007/s11665-015-1790-9 ↗
8. 10.1016/j.fusengdes.2018.10.00410.1016/j.fusengdes.2018.10.004 ↗
9. 10.1080/13621718.2017.140311010.1080/13621718.2017.1403110 ↗
10. 10.1080/13621718.2017.141524910.1080/13621718.2017.1415249 ↗
11. 10.1016/j.jmst.2019.10.00510.1016/j.jmst.2019.10.005 ↗
12. 10.1080/13621718.2019.170625910.1080/13621718.2019.1706259 ↗
13. 10.1016/j.mser.2005.07.00110.1016/j.mser.2005.07.001 ↗
14. 10.3390/met709038110.3390/met7090381 ↗
15. 10.1007/s11661-017-4413-210.1007/s11661-017-4413-2 ↗
16. 10.1016/j.jallcom.2010.05.16610.1016/j.jallcom.2010.05.166 ↗
17. 10.1016/j.msea.2015.09.11110.1016/j.msea.2015.09.111 ↗
18. 10.1016/j.fusengdes.2019.11140010.1016/j.fusengdes.2019.111400 ↗
19. 10.1016/j.jmatprotec.2020.11688010.1016/j.jmatprotec.2020.116880 ↗
20. 10.1016/j.msea.2016.07.06310.1016/j.msea.2016.07.063 ↗
21. 10.1016/j.wear.2005.04.00610.1016/j.wear.2005.04.006 ↗
22. 10.1007/s11665-019-04211-y10.1007/s11665-019-04211-y ↗
23. 10.1016/j.ijmachtools.2017.09.00210.1016/j.ijmachtools.2017.09.002 ↗
24. 10.1080/13621718.2018.147184410.1080/13621718.2018.1471844 ↗
25. 10.1016/j.scriptamat.2017.02.00910.1016/j.scriptamat.2017.02.009 ↗
26. 10.1016/j.jallcom.2017.03.06910.1016/j.jallcom.2017.03.069 ↗
27. 10.3390/met804022710.3390/met8040227 ↗
28. 10.1016/j.actamat.2012.01.03810.1016/j.actamat.2012.01.038 ↗
29. 10.1016/j.vacuum.2019.06.02710.1016/j.vacuum.2019.06.027 ↗
30. 10.1515/rams-2018-002010.1515/rams-2018-0020 ↗