Evaluation of repair welding procedures for 2.25Cr–1Mo and 9Cr–1Mo steel welds
Source abstract
Abstract
Chromium–molybdenum steels are extensively used in the steam generator circuits of power plants. These components may require welding of the cracks that can develop during fabrication, storage, and transportation stages, or during the service life of the plant. This investigation compares repair welding methods for Cr–Mo steels, using 2.25Cr–1Mo and 9Cr–1Mo materials. To simulate aging during service, welds were heat treated at 873 K for 5000 h. Simulated repair welding of the aged welds was carried out at the weld/base metal interface, i.e. at the location at which cracks are usually reported to occur during service. Two repair welding methods (half bead and butter bead temper bead methods) conforming to the ASME Boiler and Pressure Vessel Code were used. Tensile properties, hardness profiles, and X-ray diffraction based residual stress distributions were determined for both the Cr–Mo steel welds to evaluate the simulated repair welds. Analysis of the test results showed that both the repair welding methods can be used for 2.25Cr–1Mo steel welds, although the butter bead temper bead method is much more suitable for both the 2.25Cr–1Mo and 9Cr–1Mo steel welds.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Fatigue and fracture mechanics · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
the Metallurgy and Materials Group, Indira Gandhi Centre for Atomic Research, Kalpakkam 603 102, India
References (25)
Show source-provided references
1. Lundin C. D., and Wang Y. ‘Repair welding of service exposed Cr–Mo steel weldments’, Welding Research Council Project Report, University of Tennessee, Knoxville, TN, 1988.
2. Walberg G. · Weld. J · 1981 · 60 · 45
3. Kelleher K. · Weld. J · 1985 · 64 · 61
4. Anderson J. · Weld. J · 1985 · 64 · 39
5. Weld. J. 1979, 58, (2), 48.10.1016/0147-619X(79)90005-2 ↗
6. Weld. J. 1975, 54, 361.10.1049/tpe.1975.0162 ↗
7. Weld. J. 1977, 56, (5), 40–41.10.1213/00000539-197701000-00001 ↗
8. Albert S. K., Gill T. P. S., Iyer D. R., Shanmugam K., and Sampath V. P. ‘Repair welding of understraps, shrouds and blades of KAPS–1 & 2 steam turbines’, Report IGC/MJS/MTD/1/99, Indira Gandhi Centre for Atomic Research, Kalpakkam, 1999.
9. Purazrang K. · Weld. J · 1979 · 248s
10. Lacoe D. · Weld. J · 1984 · 63 · 53
11. Weld. J. 1980, 59, (2), 49–51.10.1016/0141-0296(80)90028-0 ↗
12. Delaune P. T. · Weld. J · 1987 · 66 · 32
13. Ebert H. W. · Weld. J · 1984 · 63 · 18
14. Sheward G. E. · Weld. J · 1983 · 62 · 39
15. Kiefner J. F. · Weld. J · 1977 · 56 · 26
16. Aidun D. K. · Weld. J · 1984 · 345s
17. Aidun D. K. · Weld. J · 1985 · 97s
18. Manning R. M. · Weld. J · 1983 · 62 · 27
19. Slater G. · Weld. J · 1985 · 64 · 22
20. Clark J. N. · Weld. J · 1986 · 65 · 42
21. Alberry P. J. · Weld. J · 1987 · 66 · 33
22. Boiler ASME, and Pressure Vessel Code, Section III, Division I, Articles IWB 4320–4324, ASME, New York, 1983.
23. Boiler ASME, and Pressure Vessel Code, Section XI, 217–223; Code Case N-236–1, 385–394; Code Case N - 432, 757–760, ASME, New York, 1986.
24. Noyen I. C., and Cohen J. B. ‘Residual stress measurement and interpretation by diffraction methods’; 1984, Berlin, SpringerVerlag.
25. Palanichamy P., Joseph A., Bhattacharya D. K., and Raj B. ‘Residual stresses and their evaluation in welds’, (ed. S. Sundarajan et al.), Welding Engineering Handbook, Vol. 1, 269–296; 1992, Secunderabad, Radiant Publications.