Temperature, macrostructure and hardness in high strength low alloy steel welds
Source abstract
Abstract
A series of welds have been fabricated in high strength low alloy steel (HSLA100) plate by gas metal arc welding at heat inputs of 1.0, 1.6 and 2.2 kJ mm-1. Slices from the welds were then polished and the macrostructure was observed. Hardness maps were then determined over the entire weld zone, including the heat affected zone and the base plate. Correlations were then made between the hardness maps and the macrostructure. A bead on plate weld was made using the same heat inputs and was used to determine the temperature regimes in the weld as well as thermal profiles of the weld region. Relationships showing good correlations were observed between the various microstructures, the macrostructure, the calculated thermal profiles, and the hardness values.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Moon D. W. · Weld. J · 2000 · 79 · 278s
2. Spanos G., Moon D. W., Fonda R. W., Menon E. S. K., and Fox A. G. ‘Trends in welding research’, 191–196; 1998, Materials Park, OH, ASM International.
3. 10.1179/13621710322501088010.1179/136217103225010880 ↗
4. 10.1179/13621710222500264610.1179/136217102225002646 ↗
5. Lambrakos S. G., and Moon D. W.: in ‘Computer-aided design, engineering, and manufacturing, systems techniques and applications’, Vol. 6, 6-1–6-38; 2001, New York, NY, CRC Press.
6. Andrews K. W. · J. Iron Steel Inst · 1965 · 203 · 721
7. 10.1016/0956-7151(94)90432-410.1016/0956-7151(94)90432-4 ↗
8. 10.1016/0001-6160(85)90238-X10.1016/0001-6160(85)90238-X ↗
9. Blondeau R. · ‘Heat treatment