Abstract

Aqueous batteries are regaining interest, thanks to the extended working stability voltage window in a highly concentrated electrolyte, namely the water-in-salt electrolyte. A solid-electrolyte interphase (SEI) forms on the negative electrode to prevent water access to the electrode surface. However, we further reported that the formed SEI layer was not uniform on the surface of the glassy carbon electrode. The SEI after passivation will also show degradation during the remaining time of open-circuit voltage (OCV); hence, it calls for a more stable passivation layer to cover the electrode surface. Here, a surface modification was successfully achieved via artificial diazonium grafting using monomers, such as poly(ethylene glycol), α-methoxy, ω-allyloxy (PEG), and allyl glycidyl cyclocarbonate (AGC), on glassy carbon. Physical and electrochemical measurements indicated that the hydrophobic layer composed of PEG or AGC species was well grafted on the electrode surface. The grafted hydrophobic coatings could protect the electrode surface from the water molecules in the bulk electrolyte and then suppress the free water decomposition (from LSV) but still migrating lithium ions. Furthermore, multiple cycles of CV with one-hour resting OCV identified the good stability of the hydrophobic grafting layer, which is a highlight compared with our precious work. These findings relying on the diazonium grafting design may offer a new strategy to construct a stable artificial SEI layer that can well protect the electrode surface from the free water molecule.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Advanced battery technologies research · Advancements in Battery Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

ICGM, Université de Montpellier, CNRS, 34293 Montpellier, France

College de France, 75005 Paris, France

Réseau sur le Stockage Electrochimique de l’Energie (RS2E), CNRS FR 3459, 33 rue Saint Leu, 80039 Amiens Cedex, France

Institute for Advanced Study & College of Food and Biological Engineering, Chengdu University, 610106 Chengdu, China

Molecular Electrochemistry for Energy Laboratory, School of Energy Science and Engineering, Vidyasirimedhi Institute of Science and Technology (VISTEC), 21210 Rayong, Thailand

Funding

Agence Nationale de la Recherche · Direction G?n?rale de l?Armement · National Research Council of Thailand

References (56)

Show source-provided references
1. 10.1038/s41560-017-0033-810.1038/s41560-017-0033-8 ↗
2. 10.1016/j.joule.2017.08.00910.1016/j.joule.2017.08.009 ↗
3. 10.1002/eom2.1216510.1002/eom2.12165 ↗
4. 10.1016/j.nanoen.2021.10650010.1016/j.nanoen.2021.106500 ↗
5. 10.1126/science.aab159510.1126/science.aab1595 ↗
6. 10.1002/aenm.20200244010.1002/aenm.202002440 ↗
7. 10.1038/s41467-022-33129-810.1038/s41467-022-33129-8 ↗
8. 10.1039/c9ta08699d10.1039/c9ta08699d ↗
9. 10.1021/acsenergylett.2c0001510.1021/acsenergylett.2c00015 ↗
10. 10.1016/j.mtcomm.2020.10158810.1016/j.mtcomm.2020.101588 ↗
11. 10.1002/ange.20200537810.1002/ange.202005378 ↗
12. 10.1021/acsenergylett.1c0109710.1021/acsenergylett.1c01097 ↗
13. 10.1149/2.026305jes10.1149/2.026305jes ↗
14. 10.1021/ja300224c10.1021/ja300224c ↗
15. 10.1021/ja00001a00210.1021/ja00001a002 ↗
16. 10.1021/la00060a04110.1021/la00060a041 ↗
17. 10.1021/ac50038a02010.1021/ac50038a020 ↗
18. 10.1021/cr100190410.1021/cr1001904 ↗
19. 10.1039/b406228k10.1039/b406228k ↗
20. 10.1039/c0cs00149j10.1039/c0cs00149j ↗
21. 10.3390/bios1001000410.3390/bios10010004 ↗
22. 10.1002/celc.20190104810.1002/celc.201901048 ↗
23. 10.1039/d1ay00965f10.1039/d1ay00965f ↗
24. 10.1021/la062922710.1021/la0629227 ↗
25. 10.1016/j.elecom.2007.06.01610.1016/j.elecom.2007.06.016 ↗
26. 10.1016/B978-044452224-5/50106-210.1016/B978-044452224-5/50106-2 ↗
27. 10.1002/celc.20210071210.1002/celc.202100712 ↗
28. 10.1021/acs.langmuir.9b0125410.1021/acs.langmuir.9b01254 ↗
29. 10.1016/j.apcatb.2019.03.03610.1016/j.apcatb.2019.03.036 ↗
30. 10.1021/la063235i10.1021/la063235i ↗
31. 10.1002/aenm.20200244010.1002/aenm.202002440 ↗
32. 10.1021/acs.langmuir.0c0044410.1021/acs.langmuir.0c00444 ↗
33. 10.1007/s10853-011-5709-z10.1007/s10853-011-5709-z ↗
34. 10.1021/am500582e10.1021/am500582e ↗
35. 10.4028/www.scientific.net/AMR.445.79710.4028/www.scientific.net/AMR.445.797 ↗
36. 10.1002/smll.20180190010.1002/smll.201801900 ↗
37. 10.1021/acssuschemeng.8b0558710.1021/acssuschemeng.8b05587 ↗
38. 10.1039/c2sc01034h10.1039/c2sc01034h ↗
39. 10.1007/s00339-008-4829-z10.1007/s00339-008-4829-z ↗
40. 10.1088/0957-4484/15/11/04810.1088/0957-4484/15/11/048 ↗
41. 10.1021/acsami.5b0442810.1021/acsami.5b04428 ↗
42. 10.1021/la301110310.1021/la3011103 ↗
43. 10.1016/j.cej.2022.13520710.1016/j.cej.2022.135207 ↗
44. 10.1016/S0022-0728(83)80055-210.1016/S0022-0728(83)80055-2 ↗
45. 10.1021/la202651b10.1021/la202651b ↗
46. 10.1016/S0022-0728(98)00252-610.1016/S0022-0728(98)00252-6 ↗
47. 10.1016/j.electacta.2017.12.05210.1016/j.electacta.2017.12.052 ↗
48. 10.1016/j.jelechem.2018.03.04510.1016/j.jelechem.2018.03.045 ↗
49. Bard A. J. · 2001
50. 10.1126/science.abq375010.1126/science.abq3750 ↗
51. 10.1021/acs.jpcc.1c0166310.1021/acs.jpcc.1c01663 ↗
52. 10.1021/acsenergylett.0c0034810.1021/acsenergylett.0c00348 ↗
53. 10.1002/aenm.20220072210.1002/aenm.202200722 ↗
54. 10.1016/j.electacta.2021.13849810.1016/j.electacta.2021.138498 ↗
55. 10.1039/d0nr03799k10.1039/d0nr03799k ↗
56. 10.1021/acsnano.0c0767410.1021/acsnano.0c07674 ↗