Constructing robust solid electrolyte interphase by coating Li6.4La3Zr1.4Ta0.6O12 on silicon anodes for high-performance lithium-ion batteries
Source abstract
Abstract
Silicon (Si) anodes promise attractive application prospects owing to their high theoretical specific capacity and appropriate lithiation potential. However, severe volume expansion and unstable solid electrolyte interphase (SEI) formation hinder their practical commercialization. Herein, an interface engineering strategy by coating Li6.4La3Zr1.4Ta0.6O12(LLZTO) is proposed to optimize electrochemical/mechanical properties of SEI on the Si electrode. Porous micro-spherical structure of Si@LLZTO particles promotes compactness of the electrode and alleviates volume expansion during cycling. Coating LLZTO induces Li4SiO4formation owing to the reaction of SiO2on the Si surface and Li2CO3on LLZTO. The H+/Li+exchange of LLZTO and decomposition of LiPF6are facilitated due to the presence of trace water in the electrolyte, resulting in LiF formation. The interfacial layer rich in LLZTO, LiF and Li4SiO4manipulates ion transport and volume variation of Si electrodes, inhibiting SEI rupture and regeneration. The Si@LLZTO∥Li cells deliver reversible capacity of 1961 mAh g−1with 89.1% capacity retention after 100 cycles at 1 C. The Si@LLZTO∥NCM 811 cells possess 78.6% capacity retention after 200 cycles at 0.5 C, superior to that of Si∥NCM811 cells (31.5%). The LLZTO-coating strategy with in-depth comprehension on interfacial mechanisms enlightens electrode design for high-performance Si-based lithium-ion batteries.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Extraction and Separation Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Liu T, Yang G T, Bi H, et al. Recent progress in high-energy and high-power lithium-ion batteries. Energy Storage Sci Technol, 2025, 14: 54–76
2. Yuan K, Lin Y, Li X, et al. High-Safety anode materials for advanced lithium-ion batteries. Energy & Environ Mater, 2024, 7: e1275910.1002/eem2.12759 ↗
3. Gür T M. Review of electrical energy storage technologies, materials and systems: Challenges and prospects for large-scale grid storage. Energy Environ Sci, 2018, 11: 2696–276710.1039/C8EE01419A ↗
4. Gu M, Wang Z, Connell J G, et al. Electronic origin for the phase transition from amorphous LixSi to crystalline Li15Si4. ACS Nano, 2013, 7: 6303–630910.1021/nn402349j ↗
5. Zhang L, Zhu C, Yu S, et al. Status and challenges facing representative anode materials for rechargeable lithium batteries. J Energy Chem, 2022, 66: 260–29410.1016/j.jechem.2021.08.001 ↗
6. McBrayer J D, Rodrigues M T F, Schulze M C, et al. Calendar aging of silicon-containing batteries. Nat Energy, 2021, 6: 866–87210.1038/s41560-021-00883-w ↗
7. Sun L, Liu Y, Shao R, et al. Recent progress and future perspective on practical silicon anode-based lithium ion batteries. Energy Storage Mater, 2022, 46: 482–50210.1016/j.ensm.2022.01.042 ↗
8. Wang B, Li W, Wu T, et al. Self-template construction of mesoporous silicon submicrocube anode for advanced lithium ion batteries. Energy Storage Mater, 2018, 15: 139–14710.1016/j.ensm.2018.03.025 ↗
9. Ma X, Sun D, Wang M, et al. Waste to wealth: S,N-Codoped Si/C anode derived from waste tire oil exhibits superior performance in lithium-ion batteries. ACS Sustain Chem Eng, 2024, 12: 15447–1546010.1021/acssuschemeng.4c04521 ↗
10. Cao Z, Zheng X, Wang Y, et al. Tailoring a multifunctional, boron and fluoride-enriched solid-electrolyte interphase precursor towards high-rate and stable-cycling silicon anodes. Nano Energy, 2022, 93: 10681110.1016/j.nanoen.2021.106811 ↗
11. Mu T, Sun Y, Wang C, et al. Long-life silicon anodes by conformal molecular-deposited polyurea interface for lithium ion batteries. Nano Energy, 2022, 103: 10782910.1016/j.nanoen.2022.107829 ↗
12. Chen J, Li Y, Wu X, et al. Dynamic hydrogen bond cross-linking binder with self-healing chemistry enables high-performance silicon anode in lithium-ion batteries. J Colloid Interface Sci, 2024, 657: 893–90210.1016/j.jcis.2023.12.057 ↗
13. Li H, Wang Z, Dang L, et al. Precursor induced assembly of Si nanoparticles encapsulated in graphene/carbon matrices and the influence of Al2O3 coating on their properties as anode for lithium-ion batteries. Small, 2024, 20: 230772210.1002/smll.202307722 ↗
14. Yang J, Wang Y, Li W, et al. Amorphous TiO2 shells: A vital elastic buffering layer on silicon nanoparticles for high-performance and safe lithium storage. Adv Mater, 2017, 29: 170052310.1002/adma.201700523 ↗
15. Guo F, Chen P, Kang T, et al. Silicon-loaded lithium-carbon composite microspheres as lithium secondary battery anodes. Acta Physico-Chim Sin, 2019, 35: 1365–137110.3866/PKU.WHXB201903008 ↗
16. Ding X, Liu X X, Huang Y, et al. Enhanced electrochemical performance promoted by monolayer graphene and void space in silicon composite anode materials. Nano Energy, 2016, 27: 647–65710.1016/j.nanoen.2016.07.031 ↗
17. Kim M, Ahn H, Choi J, et al. A rational design of silicon-based anode for all-solid-state lithium-ion batteries: A review. Energy Tech, 2023, 11: 220132110.1002/ente.202201321 ↗
18. Huang Y, Shao B, Wang Y, et al. Solid-state silicon anode with extremely high initial coulombic efficiency. Energy Environ Sci, 2023, 16: 1569–158010.1039/D2EE04057C ↗
19. Zhao X, Rong Y, Duan Y, et al. Development of Si-based anodes for all-solid-state Li-ion batteries. Coatings, 2024, 14: 60810.3390/coatings14050608 ↗
20. Deng Z, Chen S, Yang K, et al. Tailoring interfacial structures to regulate carrier transport in solid-state batteries. Adv Mater, 2024, 36: 240792310.1002/adma.202407923 ↗
21. Kim J, Kim C, Jang I, et al. Si nanoparticles embedded in carbon nanofiber sheathed with Li6PS5Cl as an anode material for all-solid-state batteries. J Power Sources, 2021, 510: 23042510.1016/j.jpowsour.2021.230425 ↗
22. Cao D, Ji T, Singh A, et al. Unveiling the mechanical and electrochemical evolution of nanosilicon composite anodes in sulfide-based all-solid-state batteries. Adv Energy Mater, 2023, 13: 220396910.1002/aenm.202203969 ↗
23. Liang H Z, Zhang X Y, Yang L, et al. Electrochemomechanical coupled behaviors of deformation and failure in electrode materials for lithium-ion batteries. Sci China Tech Sci, 2019, 62: 1277–129610.1007/s11431-018-9485-6 ↗
24. Huo H, Jiang M, Bai Y, et al. Chemo-mechanical failure mechanisms of the silicon anode in solid-state batteries. Nat Mater, 2024, 23: 543–55110.1038/s41563-023-01792-x ↗
25. Chen C, Li Q, Li Y, et al. Sustainable interfaces between Si anodes and garnet electrolytes for room-temperature solid-state batteries. ACS Appl Mater Interfaces, 2018, 10: 2185–219010.1021/acsami.7b16385 ↗
26. Meesala Y, Jena A, Chang H, et al. Recent advancements in Li-ion conductors for all-solid-state Li-ion batteries. ACS Energy Lett, 2017, 2: 2734–275110.1021/acsenergylett.7b00849 ↗
27. Ramakumar S, Deviannapoorani C, Dhivya L, et al. Lithium garnets: Synthesis, structure, Li+ conductivity, Li+ dynamics and applications. Prog Mater Sci, 2017, 88: 325–41110.1016/j.pmatsci.2017.04.007 ↗
28. Zhao N, Khokhar W, Bi Z, et al. Solid garnet batteries. Joule, 2019, 3: 1190–119910.1016/j.joule.2019.03.019 ↗
29. Hu C, Shen Y, Shen M, et al. Superionic conductors via bulk interfacial conduction. J Am Chem Soc, 2020, 142: 18035–1804110.1021/jacs.0c07060 ↗
30. Li W, Sun C, Jin J, et al. Realization of the Li+ domain diffusion effect via constructing molecular brushes on the LLZTO surface and its application in all-solid-state lithium batteries. J Mater Chem A, 2019, 7: 27304–2731210.1039/C9TA10400C ↗
31. Ping W, Yang C, Bao Y, et al. A silicon anode for garnet-based all-solid-state batteries: Interfaces and nanomechanics. Energy Storage Mater, 2019, 21: 246–25210.1016/j.ensm.2019.06.024 ↗
32. He Y L, Xu P, Jiang D F, et al. Quantifying the solid electrolyte interphase stress induced capacity fading of lithium-ion batteries via a multiscale mechanical-electrochemical coupling model. Sci China Tech Sci, 2024, 67: 3168–318110.1007/s11431-024-2711-7 ↗
33. Miyata N, Watanabe H, Ichikawa M. HF-chemical etching of the oxide layer near a SiO2/Si(111) interface. Appl Phys Lett, 1998, 73: 3923–392510.1063/1.122937 ↗
34. Huo H, Chen Y, Zhao N, et al. In-situ formed Li2CO3-free garnet/Li interface by rapid acid treatment for dendrite-free solid-state batteries. Nano Energy, 2019, 61: 119–12510.1016/j.nanoen.2019.04.058 ↗
35. Sharafi A, Yu S, Naguib M, et al. Impact of air exposure and surface chemistry on Li-Li7La3Zr2O12 interfacial resistance. J Mater Chem A, 2017, 5: 13475–1348710.1039/C7TA03162A ↗
36. Zhang S, Zhao H, Wang J, et al. Enhanced densification and ionic conductivity of Li-garnet electrolyte: Efficient Li2CO3 elimination and fast grain-boundary transport construction. Chem Eng J, 2020, 393: 12479710.1016/j.cej.2020.124797 ↗
37. Adnan S B R S, Mohamed N S. Citrate sol-gel synthesised Li4SiO4: Conductivity and dielectric behaviour. Mater Res Innovations, 2012, 16: 281–28510.1179/1433075X12Y.0000000012 ↗
38. Zhang J, Wang C, Zheng M, et al. Rational design of air-stable and intact anode-electrolyte interface for garnet-type solid-state batteries. Nano Energy, 2022, 102: 10767210.1016/j.nanoen.2022.107672 ↗
39. Zhang J, Yu R, Li J, et al. Transformation of undesired Li2CO3 into lithiophilic layer via double replacement reaction for garnet electrolyte engineering. Energy & Environ Mater, 2021, 5: 962–96810.1002/eem2.12222 ↗
40. Wang F, Mao J, Zhao Y. Crystal engineering of silica anode achieving intrinsic zero-strain. Adv Mater, 2023, 35: 230790810.1002/adma.202307908 ↗
41. Liu J, Gao X, Hartley G O, et al. The interface between Li6.5La3Zr1.5Ta0.5O12 and liquid electrolyte. Joule, 2020, 4: 101–10810.1016/j.joule.2019.10.001 ↗
42. Nyman M, Alam T M, McIntyre S K, et al. Alternative approach to increasing Li mobility in Li-La-Nb/Ta garnet electrolytes. Chem Mater, 2010, 22: 5401–541010.1021/cm101438x ↗
43. Leng J, Wang H, Li Y, et al. Insight into the solid-liquid electrolyte interphase between Li6.4La3Zr1.4Ta0.6O12 and LiPF6-based liquid electrolyte. Appl Surf Sci, 2022, 575: 15163810.1016/j.apsusc.2021.151638 ↗