journal article·2011-11

RETRACTED ARTICLE: TiO2 nanoparticles’ effects on properties of concrete using ground granulated blast furnace slag as binder

Ali Nazari, Shadi Riahi

This record is marked as retracted by the source. Review the publisher’s notice before using its findings.
Publisher page

Abstract

In the present study, compressive strength, pore structure, thermal behavior and microstructure characteristics of concrete containing ground granulated blast furnace slag and TiO2 nanoparticles as binder were investigated. Portland cement was replaced by different amounts of ground granulated blast furnace slag and the properties of concrete specimens were investigated. Although it negatively impacts the properties of concrete at early ages, ground granulated blast furnace slag up to 45 wt% was found to improve the physical and mechanical properties of concrete at later ages. TiO2 nanoparticles with the average particle size of 15 nm were partially added to concrete with the optimum content of ground granulated blast furnace slag and physical and mechanical properties of the specimens were measured. TiO2 nanoparticle as a partial replacement of cement up to 3 wt% could accelerate C-S-H gel formation as a result of increased crystalline Ca(OH)2 amount at the early age of hydration and hence increase compressive strength of concrete. The increased TiO2 nanoparticles’ content of more than 3 wt% may cause reduced compressive strength because of the decreased crystalline Ca(OH)2 content required for C-S-H gel formation and unsuitable dispersed nanoparticles in the concrete matrix. TiO2 nanoparticles could improve the pore structure of concrete and shift the distributed pores to harmless and less-harm pores.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Shi C, Qian J. High performance cementing materials from industrial slags: A review. Resour Conserv Recycl, 2000, 29: 195–20710.1016/S0921-3449(99)00060-9 ↗
2. Smith M A. The economic and environmental benefits of increased use of pfa and granulated slag. Resour Policy, 1975, 1(3): 154–17010.1016/0301-4207(75)90030-6 ↗
3. Collins R J, Ciesielski S K. Recycling and Use of Waste Materials and By-Products in Highway Construction. National Cooperative Highway Research Program Synthesis of Highway Practice 199. Washington DC: Transportation Research Board, 1994
4. Afrani I, Rogers C. The effects of different cementing materials and curing on concrete scaling. Cement Concrete Aggregates, 1994, 16: 132–13910.1520/CCA10291J ↗
5. Malhotra V M. Properties of fresh and hardened concrete incorporating ground granulated blast furnace slag. In: Malhotra V M, ed. Supplementary Cementing Materials for Concrete. Canada: Minister of Supply and Services, 1987. 291–33610.4095/305059 ↗
6. Isozaki K. Some properties of alkali-activated slag cements. CAJ Rev, 1986: 120–123
7. Deng Y, Wu X, Tang M. High strength alkali-slag cement. J Nanjing Inst Chem Technol, 1989: 11(2): 1–7
8. Shi C, Wu X, Tang M. Hydration of alkali-slag cements at 150°C. Cem Concr Res, 1991, 21: 91–10010.1016/0008-8846(91)90035-G ↗
9. Deja J, Malolepszy J. Resistance of alkali-activated slag mortars to chloride solution. In: Proceedings of the Third International Conference on the Use of Fly Ash, Silica Fume, Slag and Natural Pozzolans in Concrete, SP-114, American Concrete Institute, Norway, Chicago, 1989. 1547–1561
10. Shi C, Shen X, Wu X, et al. Immobilization of radioactive wastes with Portland and alkali-slag cement pastes. Cemento, 1994, 91(2): 97–108
11. Siliceous By-products for Use in Concrete. Final Report of the 73 BSC RILEM Committee, 1988
12. Sohaib M M, Ahmed S A, Balaha M M. Effect of fire and cooling mode on the properties of slag mortars. Cem Concr Res, 2001, 31(11): 1533–153810.1016/S0008-8846(01)00561-0 ↗
13. Detwiler R J, Fapohunda C A, Natale J. Use of supplementary cementing materials to increase the resistance to chloride ion penetration of concretes cured at elevated temperatures. ACI Mater J, 1994, 91(1): 63–66
14. Ramlochan T, Zacarias P, Thomas M D A, et al. The effect of pozzolans and slag on the expansion of mortars cured at elevated temperature: Part I expansive behaviour. Cem Concr Res, 2003, 33(6): 807–81410.1016/S0008-8846(02)01066-9 ↗
15. Bleszynski R F, Hooton R D, Thomas M D A, et al. Durability of ternary blend concretes with silica fume and blast furnace slag: Laboratory and outdoor exposure site studies. ACI Mater J, 2002, 99(5): 499–508
16. Qing Y, Zenan Z, Deyu K, et al. Influence of nano-SiO2 addition on properties of hardened cement paste as compared with silica fume. Constr Build Mat, 2007, 21: 539–54510.1016/j.conbuildmat.2005.09.001 ↗
17. Jo B W, Kim C H, Tae G H, et al. Characteristics of cement mortar with nano-SiO2 particles. Constr Build Mat, 2007, 21: 1351–135510.1016/j.conbuildmat.2005.12.020 ↗
18. Jo B W, Kim C H, Lim J H. Investigations on the development of powder concrete with nano-SiO2 nanoparticles. KSCE J, 2007, 11(1): 37–4210.1007/BF02823370 ↗
19. Jo B W, Kim C H, Lim J H. Characteristics of cement mortar with nano-SiO2 particles. ACI Mater J, 2007, 104(7): 404–407
20. Lin K L, Chang W C, Linc D F, et al. Effects of nano-SiO2 and different ash nanoparticle sizes on sludge ash-cement mortar. J Env Manag, 2008, 8(4): 708–71410.1016/j.jenvman.2007.03.036 ↗
21. Lin D F, Lin K L, Chang W C, et al. Improvements of nano-SiO2 on sludge/fly ash mortar. Waste Manage, 2008, 28(6): 1081–108710.1016/j.wasman.2007.03.023 ↗
22. Shih J Y, Chang T P, Hsiao T C. Effect of nanosilica on characteriza tion of Portland cement composite. Cem Con Res, 2006, 36: 697–70610.1016/j.cemconres.2005.11.006 ↗
23. Campillo I, Guerrero A, Dolado J S, et al. Improvement of initial mechanical strength by nanoalumina in belite cements. Mater Lett, 2007, 61: 1889–189210.1016/j.matlet.2006.07.150 ↗
24. Li Z, Wang H, He S, et al. Investigations on the preparation and mechanical properties of the nano-alumina reinforced cement composite. Mater Lett, 2006, 60: 356–35910.1016/j.matlet.2005.08.061 ↗
25. Li H, Xiao H, Ou J. A study on mechanical and pressure-sensitive properties of cement mortar with nanophase materials. Cem Con Res, 2004, 34: 435–43810.1016/j.cemconres.2003.08.025 ↗
26. Flores-Velez L M, Dominguez O. Characterization and properties of Portland cement composites incorporating zinc-iron oxide nanoparticles. J Mater Sci, 2002, 37: 983–98810.1023/A:1014304131987 ↗
27. Nazari A, Riahi S. Microstructural, thermal, physical and mechanical behavior of the self compacting concrete containing SiO2 nanoparticles. Mater Sci Eng A, 2010, 527: 7663–767210.1016/j.msea.2010.08.095 ↗
28. Nazari A, Riahi S. The effects of TiO2 nanoparticles on flexural damage of self-compacting concrete. Int J Damage Mech, 2010, doi: 10.1177/105678951038526210.1177/1056789510385262 ↗
29. Nazari A, Riahi S. The effect of TiO2 nanoparticles on water permeability and thermal and mechanical properties of high strength self-compacting concrete. Mater Sci Eng A, 2010, 528(2): 756–76310.1016/j.msea.2010.09.074 ↗
30. Nazari A. The effects of curing medium on flexural strength and water permeability of concrete incorporating TiO2 nanoparticles. Mater Struct, 2010, doi: 10.1617/s11527-010-9664-y10.1617/s11527-010-9664-y ↗
31. Nazari A, Riahi S. The effects of zinc dioxide nanoparticles on flexural strength of self-compacting concrete. Compos Part B-Eng, 2011, 42(2): 167–17510.1016/j.compositesb.2010.09.001 ↗
32. Nazari A, Riahi S. The effects of ZnO2 nanoparticles on split tensile strength of self-compacting concrete. J Exp Nanosc, 2010, doi: 10.1080/17458080.2010.52466910.1590/S1516-14392010000400011 ↗
33. Nazari A, Riahi S. Limewater effects on properties of ZrO2 nanoparticle blended cementitious composite. J Compos Mater, 2010, doi: 10.1177/002199831037611810.1177/0021998310376118 ↗
34. Nazari A, Riahi S. Assessment of the effects of Fe2O3 nanoparticles on water permeability, workability, and setting time of concrete. J Compos Mater, 2010, doi: 10.1177/002199831037794510.1177/0021998310377945 ↗
35. Nazari A, Riahi S. The effects of limewater on flexural strength and water permeability of Al2O3 nanoparticles binary blended concrete. J Compos Mater, 2010, doi: 10.1177/002199831037890710.1177/0021998310378907 ↗
36. Nazari A, Riahi S. The effects of limewater on split tensile strength and workability of Al2O3 nanoparticles binary blended concrete. J Compos Mater, 2010, doi: 10.1177/002199831037890910.1177/0021998310378909 ↗
37. Nazari A, Riahi S. The effects of TiO2 nanoparticles on properties of binary blended concrete. J Compos Mater, 2010, doi: 10.1177/002199831037891010.1177/0021998310378910 ↗
38. Nazari A, Riahi S. Optimization mechanical properties of Cr2O3 nanoparticle binary blended cementitious composite. J Compos Mater, 2010, doi: 10.1177/002199831037794410.1177/0021998310377944 ↗
39. Li H, Zhang M H, Ou J P. Flexural fatigue performance of concrete containing nano-nanoparticles for pavement. Int J Fatigue, 2007, 29: 1292–130110.1016/j.ijfatigue.2006.10.004 ↗
40. Li H, Zhang M H, Ou J P. Abrasion resistance of concrete containing nano-nanoparticles for pavement. Wear, 2006, 260: 1262–126610.1016/j.wear.2005.08.006 ↗
41. Katyal N K, Ahluwalia S C, Parkash R. Effect of TiO2 on the hydration of tricalcium silicate. Cem Con Res, 1999, 29: 1851–185510.1016/S0008-8846(99)00171-4 ↗
42. ASTM C150, Standard Specification for Portland Cement, Annual Book of ASTM Standards. Philadelphia, PA: ASTM, 2001
43. ASTM C39, Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens, Philadelphia, PA: ASTM, 2001
44. Abell A B, Willis K L, Lange D A. Mercury intrusion porosimetry and image nalysis of cement-based materials. J Colloid Interface Sci, 1999, 211: 39–4410.1006/jcis.1998.5986 ↗
45. Tanaka K, Kurumisawa K. Development of technique for observing pores in hardened cement paste. Cem Con Res, 2002, 32: 1435–144110.1016/S0008-8846(02)00806-2 ↗
46. Roncero J, Gettu R. Influencia de los superplastificantes en la microestructura de la pasta hidratada y en el comportamiento diferido de los morteros de cemento. Cemento Hormigón, 2002, 832: 12–28
47. Hans-Ërik G, Pentti P. Properties of SCC-especially early age and long term shrinkage and salt frost resistance. Proceedings of the 1st international RILEM symposium on self-compacting concrete, RILEM Publications S.A.R.L.; Stockholm, 1999. 211–225
48. Song H W, Byun K J, Kim S H, et al. Early-age creep and shrinkage in self-compacting concrete incorporating GGBFS. Proceedings of the 2nd international RILEM symposium on self-compacting concrete. Tokyo: COMS Engineering Corporation, 2001. 413–422
49. Hammer T A, Johansen K, Bjøntegaard Ø. Volume changes as driving forces to self-induced cracking of norwegian SCC. Proceedings of the 2nd international RILEM symposium on self-compacting concrete. Tokyo: COMS Engineering Corporation, 2001. 423–432
50. Turcry P, Loukili A. A study of plastic shrinkage of self-compacting concrete, Proceedings of the 3rd International RILEM Symposium on Self-Compacting Concrete. RILEM Publications S.A.R.L.; Reykjavik, 2003. 576–585
51. Heirman G, Vandewalle L. The influence of fillers on the properties of self-compacting concrete in fresh and hardened state. Proceedings of the 3rd International RILEM Symposium on Self-Compacting Concrete. RILEM Publications S.A.R.L.; Reykjavik, 2003. 606–618
52. Ye G, Xiu X, De Schutter G, et al. Influence of limestone powder as filler in SCC on hydration and microstructure of cement pastes. Cem Con Compos, 2007, 29(2): 94–10210.1016/j.cemconcomp.2006.09.003 ↗
53. Arya C, Xu Y. Effect of cement type on chloride binding and corrosion of steel in concrete. Cem Concr Res, 1995, 25(4): 893–90210.1016/0008-8846(95)00080-V ↗
54. Polder R B, de Rooij. Durability of marine concrete structures-field investigations and modeling. Heron, 2005, 50(3): 133–153
55. Glass G K, Reddy B, Buenfeld N R. Corrosion inhibition in concrete arising from its acid neutralization capacity. Corros Sci, 2000, 42: 1587–159810.1016/S0010-938X(00)00008-1 ↗
56. Basheer P A M, Gilleece P R V, Long A E, et al. Monitoring electrical resistance of concretes containing alternative cementitious materials to assess their resistance to chloride penetration. Cem Concr Compos, 2002, 24: 437–44910.1016/S0958-9465(01)00075-0 ↗
57. Puertas F, Santos H, Palacios M, et al. Polycarboxylate superplasticiser admixtures: Effect on hydration, microstructure and rheological behavior. Adv Cem Res, 2005, 17(2): 77–8910.1680/adcr.2005.17.2.77 ↗
58. Jawed J, Skalny J, Young J F. Hydration of Portland Cement. Structure and Performance of Cements. Barnes P, ed. Essex: Applied Science Publishers, 1983. 284–285
59. Kondo R, Yoshida K. Miscibility of special elements in tricalcium silicate and alite and the hydration properties of C3S solid solutions. 5th Int Symp on the Chem of Cement, Tokyo, I-262. 1968
60. Teoreanu I, Muntean M, Balusoiu H. Addition of titanium dioxide to Portland cement clinkers. Il Cemento, 1987. 497–404
61. Kondo R, Ueda S. Kinetics of hydration of cements. 5th Int Symp on the Chem of Cement, Part 2, 1968. 211