journal article·2013-06

Slurry erosion behaviors of P110 steel and chromizing coating in liquid-solid two-phase flow

NaiMing Lin, FaQin Xie, JiaoJuan Zou, Bin Tang

Publisher page

Abstract

A chromizing coating was formed on P110 oil casing tube steel (P110 steel) via pack cementation to improve its performance and increase the lifetime during operation. The slurry erosion behaviors of the P110 steel substrate and the chromizing coating were assessed in a liquid-solid two-phase flow condition. The results showed that the obtained coating exhibited higher surface hardness, lower mass loss, and lower slurry erosion rate than those of P110 steel. The chromizing treatment has significantly improved the surface hardness and slurry erosion resistance of P110 steel.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Erosion and Abrasive Machining · High-Temperature Coating Behaviors · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Li H L, Zhang Y P, Han L H. Development situation of OCTG and production localization of hi-grade OCTG-Part I (in Chinese). Steel Pipe, 2007, 36(6): 1–6
2. Li H L, Zhang Y P, Han L H. Development situation of OCTG and production localization of hi-grade OCTG-Part II (in Chinese). Steel Pipe, 2008, 37(1): 1–6
3. Inaba H, Kimura M, Yokokawa H. An analysis of the corrosion resistance of low chromium-steel in a wet CO2 environment by the use of an electrochemical potential diagram. Corros Sci, 1996, 38: 1449–146110.1016/0010-938X(96)00032-7 ↗
4. Cai Y D, Guo P C, Liu D M, et al. Comparative study on CO2 corrosion behavior of N80, P110, X52 and 13Cr pipe lines in simulated stratum water. Sci China Tech Sci, 2010, 53: 2342–234910.1007/s11431-010-3093-6 ↗
5. Moreira R M, Franco C V, Joia C J B M, et al. The effects of temperature and hydrodynamics on the CO2 corrosion of 13Cr and 13Cr5Ni2Mo stainless steels in the presence of free acetic acid. Corros Sci, 2004, 46: 2987–300310.1016/j.corsci.2004.05.020 ↗
6. Carvalho D S, Joia C J B, Mattos O R. Corrosion rate of iron and iron-chromium alloys in CO2 medium. Corros Sci, 2005, 47: 2974–298610.1016/j.corsci.2005.05.052 ↗
7. Pfennig A, Bäßler R. Effect of CO2 on the stability of steels with 1% and 13% Cr in saline water. Corros Sci, 2009, 51: 931–94010.1016/j.corsci.2009.01.025 ↗
8. Liu X, Zheng Y G, Okafor P C. Carbon dioxide corrosion inhibition of N80 carbon steel in single liquid phase and liquid/particle two-phase flow by hydroxyethyl imidazoline derivatives. Mater Corros, 2009, 60: 507–51310.1002/maco.200805133 ↗
9. Schroeder R M, Müller I L. Fatigue and corrosion fatigue behavior of 13Cr and duplex stainless steel and a welded nickel alloy employed in oil and gas production. Mater Corros, 2009, 60: 365–37110.1002/maco.200805093 ↗
10. Migahed M A, Nassar I F. Corrosion inhibition of tubing steel during acidization of oil and gas wells. Electrochim Acta, 2008, 53: 2877–288210.1016/j.electacta.2007.10.070 ↗
11. Ren C Q, Liu D X, Bai Z Q, et al. Corrosion behavior of oil tube steel in stimulant solution with hydrogen sulfide and carbon dioxide. Mater. Chem Phys, 2005, 93: 305–309
12. Okafor P C, Liu X, Zheng Y G. Corrosion inhibition of mild steel by ethylamino imidazoline derivative in CO2-saturated solution. Corros Sci, 2009, 51: 761–76810.1016/j.corsci.2009.01.017 ↗
13. Nešić S. Key issues related to modelling of internal corrosion of oil and gas pipelines—A review. Corros Sci, 2007, 49: 4308–433810.1016/j.corsci.2007.06.006 ↗
14. Lv X H, Zhao G X, Zhang J B, et al. Research progress in low Cr corrosion resistant tubular materials (in Chinese). Mater Rev, 2009, 23: 72–76
15. Hu X M, Neville A. CO2 erosion-corrosion of pipeline steel (API X65) in oil and gas conditions—A systematic approach. Wear, 2009, 267: 2027–203210.1016/j.wear.2009.07.023 ↗
16. Schmitt G, Bakalli M. Advanced models for erosion corrosion and its mitigation. Mater Corros, 2008, 59: 181–19210.1002/maco.200804153 ↗
17. Akinci A, Ercenk E, Yilmaz S, et al. Slurry erosion behaviors of basalt filled low density polyethylene composites. Mater Design 2011, 32: 3106–311110.1016/j.matdes.2010.12.029 ↗
18. Thakur L, Arora N, Jayaganthan R, et al. An investigation on erosion behavior of HVOF sprayed WC-CoCr coatings. Appl Surf Sci, 2011, 258: 1225–123410.1016/j.apsusc.2011.09.079 ↗
19. Suchánek J, Kuklík V, Zdravecká E. Influence of microstructure on erosion resistance of steels. Wear, 2009, 267: 2092–209910.1016/j.wear.2009.08.004 ↗
20. Ribeiro L M F, Horovistiz A L, Jesuíno G A, et al. Fractal analysis of eroded surfaces by digital image processing. Mater Lett, 2002, 56: 512–51710.1016/S0167-577X(02)00542-6 ↗
21. Purandare Y, Stack M M, Hovsepian P. A study of the erosion-corrosion of PVD CrN/NbN superlattice coatings in aqueous slurries. Wear, 2005, 259: 256–26210.1016/j.wear.2005.01.047 ↗
22. Wang H W, Stack M M, Lyon SB, et al. Wear associated with growth defects in combined cathodic arc/unbalanced magnetron sputtered CrN/NbN superlattice coatings during erosion in alkaline slurry. Surf Coat Technol, 2000, 135: 82–9010.1016/S0257-8972(00)00913-0 ↗
23. Babu P S, Basu B, Sundararajan G. The influence of erodent hardness on the erosion behavior of detonation sprayed WC-12Co coatings. Wear, 2011, 270: 903–91310.1016/j.wear.2011.02.019 ↗
24. Subramanian B, Muraleedharan C V, Ananthakumar R, et al. A comparative study of titanium nitride (TiN), titanium oxy nitride (TiON) and titanium aluminum nitride (TiAlN), as surface coatings for bio implants. Surf Coat Technol, 2011, 205: 5014–502010.1016/j.surfcoat.2011.05.004 ↗
25. Rodríguez E, Flores M, Pérez A, et al. Erosive wear by silica sand on AISI H13 and 4140 steels. Wear, 2009, 267: 2109–211510.1016/j.wear.2009.08.009 ↗
26. Tushinsky L, Kovensky I, Plokhov A, et al. Coated Metal Structure and Properties of Metal Coating Compositions. Berlin: Springer, 2002. 251
27. Mellor B G. Surface Coatings for Protection Against Wear. Cambridge: Woodhead Publishing Ltd, 2006. 79
28. Lin N M, Xie F Q, Zhong T, et al. Review on the development and prospect of surface protection technology for oil casing tubes (in Chinese). Corros Prot, 2009, 30: 801–805
29. Lin N M, Xie F Q, Zhong T, et al. Influence of adding various rare earths on microstructures and corrosion resistance of chromizing coatings prepared via pack cementation on P110 steel. J Raer Earth, 2010, 28: 301–30410.1016/S1002-0721(09)60101-0 ↗
30. Wang Z B, Lu J, Lu K. Chromizing behaviors of a low carbon steel processed by means of surface mechanical attrition treatment. Acta Mater, 2005, 53: 2081–208910.1016/j.actamat.2005.01.020 ↗
31. Lin N M, Xie F Q, Zhou J, et al. Corrosion behaviors of P110 steel and chromium coating in CO2-saturated simulated oilfield brine. J Wuhan Univer Technol Mater Sci Ed, 2011, 26: 191–197
32. Lee S B, Cho K H, Lee W G, et al. Improved corrosion resistance and interfacial contact resistance of 316L stainless-steel for proton exchange membrane fuel cell bipolar plates by chromizing surface treatment. J Power Sour, 2009, 187: 318–32310.1016/j.jpowsour.2008.11.064 ↗
33. Tsipas S A, Omar H, Perez F H, et al. Boroaluminide coatings on ferritic-martensitic steel deposited by low-temperature pack cementation. Surf Coat Technol, 2008, 202: 3263–327110.1016/j.surfcoat.2007.11.034 ↗
34. Peng X M, Xia C Q, Liu Y Y, et al. Surface molybdenizing on titanium by halide-activated pack cementation. Surf Coat Technol, 2009, 203: 3306–331010.1016/j.surfcoat.2009.04.008 ↗
35. Xu C, Peng X, Zheng L, et al. Erosion-corrosion in a laboratory-scale coal-firing FBC of various aluminized coatings prepared by low-temperature pack cementation. Surf Coat Technol, 2011, 205: 4540–454610.1016/j.surfcoat.2011.03.117 ↗
36. Vourlias G, Pistofidis N, Chaliampalias D, et al. Zinc deposition with pack cementation on low carbon steel substrates. J Alloy Compd, 2006, 416: 125–13010.1016/j.jallcom.2005.08.037 ↗
37. Lin N M, Xie F Q, Wu X Q, et al. Influence of process parameters on thickness and wear resistance of rare earth modified chromium coatings on P110 steel synthesized by pack cementation. J Rare Earth, 2011, 29: 396–40010.1016/S1002-0721(10)60467-X ↗
38. Chen C F. Research on electro-chemical behavior and corrosion scale characteristics of CO2 corrosion for tubing and casing steel. Dissertation for the Doctoral Degree. Xi’an: Northwestern Polytchnical University, 2002. 21
39. Li P. Study on erosion-corrosion behavior of stainless steel in acidic liquid-solid two-phase flow. Dissertation for the Doctoral Degree. Wuhan: Huazhong University of Science and Technology, 2006. 19
40. Guo N, Liu Q, Xin Y C, et al. The application of back-scattered electron imaging for characterization of pearlitic steels. Sci China Tech Sci, 2011, 54: 2368–237210.1007/s11431-011-4500-3 ↗
41. Qi T, Guo X P. Structure formation of Si-Y2O3 co-deposition coatings on Nb-silicide-based alloy (in Chinese). The Chin J Nonferr Met, 2009, 19: 1822–1828
42. Lin N M, Xie F Q, Zhou J, et al. Microstructures and wear resistance of chromium coatings on P110 steel fabricated by pack cementation. J Central South Univer, 2010, 17: 1155–116210.1007/s11771-010-0612-3 ↗
43. Xi Y T, Liu D X, Han D. Improvement of erosion and erosion-corrosion resistance of AISI420 stainless steel by low temperature plasma nitriding. Appl Surf Sci, 2008, 254: 5953–595810.1016/j.apsusc.2008.03.189 ↗
44. Shangguan Q Q, Cheng X H. Effect of rare earth elements on erosion resistance of nitrocarburized layers of 38CrMoAl steel. J Rare Earth, 2004, 22: 406–409
45. Xu J, Zhuo C Z, Jiang S Y. Effect of nanoparticles on the erosion-corrosion resistance property of a Ni-based alloying layer (in Chinese). Acta Phys-Chim Sin, 2009, 25: 1958–196610.3866/PKU.WHXB20090921 ↗
46. Bao C G, Gao Y M, Xing J D. Interaction between erosive-wear and corrosion of alloy materials for hydroturbine in hydroelectric station (in Chinese). J Xi’an Jiaotong Univer, 2010, 44: 66–70
47. Xu J, Zhuo C Z, Han D Z, et al. Effect of nano-Al2O3 on erosion-corrosion behaviour of composite alloying layer under two phase flow conditions. Corros Eng Sci Technol, 2011, 46: 285–29510.1179/174327809X409178 ↗
48. Xu J, Zhou C, Chen Z F, et al. Corrosion behaviors of (Cr,Fe)3Si/Cr13Fe5Si2 composite coating under condition of synergistic effects of electrochemical corrosion and mechanical erosion. J Alloy Compd, 2010, 496: 429–43210.1016/j.jallcom.2010.01.156 ↗
49. Xu J, Zhuo C. Erosion-corrosion characteristic of nano-particulates reinforced Ni-Cr-Mo-Cu surface alloying layer in acidic flow and acidic slurry flow. Mater Corros, 2010, 61: 7–1510.1002/maco.200905235 ↗
50. Ahmad Z, Abdul Aleem B J. Resistance of nanostructured titanium dioxide coatings to erosion corrosion. Tribol-Mater Surf Interf, 2009, 3: 41–4810.1179/175158309X419070 ↗
51. Guilemany J M, Torrell M, Miguel J R. Erosion corrosion properties of HVOF coatings for municipal solid waste incinerator protection. Corros Eng Sci Technol, 2008, 43: 38–4510.1179/174327807X234651 ↗
52. Recco A A C, López D, Bevilacqua A F, et al. Improvement of the slurry erosion resistance of an austenitic stainless steel with combinations of surface treatments: Nitriding and TiN coating. Surf Coat Technol, 2007, 202: 993–99710.1016/j.surfcoat.2007.07.078 ↗
53. Liu Y, Long Y Q, Liu P, et al. Erosion wear behavior of Cu-Cr-Zr alloy in liquid-solid two-phase flow (in Chinese). The Chin J Nonferr Met, 2007, 17: 1650–1655
54. Liu B L, Wu X X, Gao D L, et al. Effects of FeSi75 addition on liquid-solid flow erosion-wear resistance of sialon-Si3N4-SiC composites (in Chinese). Rare Met Mater Eng, 2009, 38: S681–S684
55. He S Z, Huang X M, Zheng H M, et al. Research on wear behavior of Ni-Cu-P coating in different mediums (in Chinese). Tribology, 2009, 29: 362–367