Abstract

Nickel-based superalloy (GH4169) is an ideal material for preparing turbine blades. Profile grinding of the fir-tree-shaped turbine blade root can easily cause thermal damage to the workpiece specimen. This study aims to enhance the suppression of alloy thermal damage by regulating the thickness of the oxide film on the cubic boron nitride (CBN) grinding wheel during the electrolytic in-process dressing (ELID)-assisted grinding process. A theoretical model for calculating the thickness of oxide film in ELID-assisted grinding was developed. Finite element simulation was conducted using the electrolytic film-forming process of the grinding wheel. The effects of electrical/nonelectrical parameters on the oxide film characteristics and grinding responses were addressed. The optimal matching scheme of process parameters was established. The results showed that the film layer of the grinding wheel at the blade root cam is more seriously damaged, and the workpiece surface is rougher. Further optimization of the electrode is demanded to achieve different dressing effects at various positions of the grinding wheel based on the workpiece profile. By reducing the interelectrode gap (he), increasing the power supply voltage (Eo), and controlling the electrolysis time (Δt) at 10–15 min, the preferred film-forming efficiency and grinding quality can be achieved. By increasing the grinding wheel speed (Vs) or decreasing the workpiece feed rate (Vf) and grinding depth (ap), the grinding thermal damage can be suppressed. A larger value ofVforapcan be selected to acquire a compromise between grinding quality and film-forming efficiency after increasing the value ofVs. The optimal combination of electrical and nonelectrical parameters during this test isEo= 120 V, Δt= 15 min,he= 0.1 mm,Vf= 50 mm min−1,Vs= 30 m s−1, andap= 0.4 mm.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced machining processes and optimization · Advanced Surface Polishing Techniques · Advanced Machining and Optimization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Soo S L, Hood R, Aspinwall D K, et al. Machinability and surface integrity of RR1000 nickel based superalloy. CIRP Ann, 2011, 60: 89–9210.1016/j.cirp.2011.03.094 ↗
2. Klocke F, Klink A, Veselovac D, et al. Turbomachinery component manufacture by application of electrochemical, electro-physical and photonic processes. CIRP Ann, 2014, 63: 703–72610.1016/j.cirp.2014.05.004 ↗
3. Pollock T M, Tin S. Nickel-based superalloys for advanced turbine engines: Chemistry, microstructure and properties. J Propulsion Power, 2006, 22: 361–37410.2514/1.18239 ↗
4. Thrinadh J, Mohapatra A, Datta S, et al. Machining behavior of Inconel 718 superalloy: Effects of cutting speed and depth of cut. Mater Today-Proc, 2020, 26: 200–20810.1016/j.matpr.2019.10.128 ↗
5. Li Y, Wang L, Zhang G, et al. Creep deformation related to ′ phase cutting at high temperature of a [111] oriented nickel-base single crystal superalloy. Mater Sci Eng-A, 2019, 763: 138162–13816910.1016/j.msea.2019.138162 ↗
6. Yin Y, Chen M. Analysis of grindability and surface integrity in creep-feed grinding of high-strength steels. Materials, 2024, 17: 1784–180210.3390/ma17081784 ↗
7. Gao S, Yang C, Xu J, et al. Wear behavior of monolayer-brazed CBN wheels with small diameter during internal traverse grinding. Int J Adv Manuf Technol, 2018, 94: 1221–122810.1007/s00170-017-0875-z ↗
8. Saleh T, Rahman M. 11.18 Electrolytic In-Process Dressing (ELID) grinding for nano-surface generation. Comp Mater Process, 2014, 11: 483–52210.1016/B978-0-08-096532-1.01112-2 ↗
9. Yang L, Ren C, Jin X. Experimental study of ELID grinding based on the active control of oxide layer. J Mater Process Tech, 2010, 210: 1748–175310.1016/j.jmatprotec.2010.06.005 ↗
10. Wang Z, Ren C, Chen G, et al. A comparative study on state of oxide layer in ELID grinding with tool-cathode and workpiece-cathode. Int J Adv Manuf Technol, 2018, 94: 1299–130710.1007/s00170-017-0931-8 ↗
11. Li X, Guan C, Zhao P. Influences of milling and grinding on machined surface roughness and fatigue behavior of GH4169 superalloy workpieces. Chin J Aeronautics, 2018, 31: 1399–140510.1016/j.cja.2017.07.013 ↗
12. Wu Q P, Wang Y, Qu W, et al. Research status and perspectives of ELID grinding fluid. China Mech Eng, 2017, 28: 1118–1126
13. Ren C, Li X, Wu M. A grinding force model considering the arc-track feeding unit device in ELID grinding of the non-standard ultra-precision bearings. J Manuf Processes, 2023, 108: 38–4710.1016/j.jmapro.2023.10.057 ↗
14. Wu J, Yu G, Gao Y, et al. Mechatronics modeling and vibration analysis of a 2-DOF parallel manipulator in a 5-DOF hybrid machine tool. Mechanism Machine Theor, 2018, 121: 430–44510.1016/j.mechmachtheory.2017.10.023 ↗
15. Wu J, Wang J, Wang L, et al. Study on the stiffness of a 5-DOF hybrid machine tool with actuation redundancy. Mechanism Machine Theor, 2009, 44: 289–30510.1016/j.mechmachtheory.2008.10.001 ↗
16. Rahman M, Senthil Kumar A, Biswas I. A review of electrolytic in-process dressing (ELID) grinding. Key Eng Mater, 2009, 404: 45–5910.4028/www.scientific.net/KEM.404.45 ↗
17. Tang K. Study on mechanism and experiment of ELID grinding based on nozzle electrolysis. Dissertation for the Doctoral Degree. Changsha: Hunan University, 2013. 1–195
18. Zhang K, Ren C, Yang L, et al. Precision internal grinding of bearing steel based on the state control of oxide layer with electrolytic in-process dressing. J Mater Process Tech, 2012, 212: 1611–162110.1016/j.jmatprotec.2012.02.018 ↗
19. Chen F, Li G, Zhao B, et al. Thermomechanical coupling effect on characteristics of oxide film during ultrasonic vibration-assisted ELID grinding ZTA ceramics. Chin J Aeronautics, 2021, 34: 125–14010.1016/j.cja.2020.05.039 ↗
20. Miao Q, Ding W, Kuang W, et al. Comparison on grindability and surface integrity in creep feed grinding of GH4169, K403, DZ408 and DD6 nickel-based superalloys. J Manuf Processes, 2020, 49: 175–18610.1016/j.jmapro.2019.11.027 ↗
21. Chen S G, Yu Z Q, Liu J W, et al. Simulation analysis and experimental research on micro-pits of mask electrochemical machining. Mach Des Manuf, 2018, 8: 155–178
22. Fang X L. Research on key techniques of shaped tube electrochemical machining. Dissertation for the Doctoral Degree. Nanjing: Nanjing University of Aeronautics and Astronautics, 2013. 1–138
23. Deconinck D, Van Damme S, Albu C, et al. Study of the effects of heat removal on the copying accuracy of the electrochemical machining process. Electrochim Acta, 2011, 56: 5642–564910.1016/j.electacta.2011.04.021 ↗
24. Gao T, Zhang X, Li C, et al. Surface morphology evaluation of multi-angle 2D ultrasonic vibration integrated with nanofluid minimum quantity lubrication grinding. J Manuf Processes, 2020, 51: 44–6110.1016/j.jmapro.2020.01.024 ↗
25. Alqahtani B, Zhang M, Marinescu I, et al. Microscopic characterization and modeling of oxide layer for electrolytic in-process dressing (ELID) grinding with focus on voltage, electrode-wheel gap, and coolant flow. Int J Adv Manuf Technol, 2019, 105: 4853–486210.1007/s00170-019-03435-5 ↗
26. Wu M L, Zhang K, Ren C. Study on the non-uniform contact during ELID groove grinding. Precision Eng, 2015, 39: 116–12410.1016/j.precisioneng.2014.07.011 ↗
27. Yin Y, Xu J, Shi L, et al. Study on thermal damage formation mechanisms and surface integrity in creep-feed profile grinding of superalloys. J Manuf Processes, 2024, 120: 28–5010.1016/j.jmapro.2024.03.114 ↗
28. Zhao Q, Guo B. Ultra-precision grinding of optical glasses using mono-layer nickel electroplated coarse-grained diamond wheels. Part 1: ELID assisted precision conditioning of grinding wheels. Precision Eng, 2015, 39: 56–6610.1016/j.precisioneng.2014.07.006 ↗
29. Dang J, Li Y, Zhang X, et al. Surface fatigue characterization and its enhancement by the engineered ultrasonic rolling process for 300 M ultrahigh strength steel. Theor Appl Fract Mech, 2024, 134: 104707–10472410.1016/j.tafmec.2024.104707 ↗
30. Zhao Q, Guo B. Ultra-precision grinding of optical glasses using mono-layer nickel electroplated coarse-grained diamond wheels. Part 2: Investigation of profile and surface grinding. Precision Eng, 2015, 39: 67–7810.1016/j.precisioneng.2014.07.007 ↗
31. Xiao Q, Qian X M, Shen Y B. Study on the experiment of ELID grinding of carbide ally. Manuf Techn Mach Tool, 2007, 4: 75–79
32. Klocke F, Thiermann J, Mattfeld P. Influence of the dressing process on grinding wheel wear. Prod Eng Res Dev, 2015, 9: 563–56810.1007/s11740-015-0606-y ↗
33. Souza A M, da Silva E J. Global strategy of grinding wheel performance evaluation applied to grinding of superalloys. Precision Eng, 2019, 57: 113–12610.1016/j.precisioneng.2019.03.013 ↗
34. Ruzzi R S, da Silva R B, da Silva L R R, et al. Influence of grinding parameters on Inconel 625 surface grinding. J Manuf Processes, 2020, 55: 174–18510.1016/j.jmapro.2020.04.002 ↗
35. Sinha M K, Setti D, Ghosh S, et al. An investigation on surface burn during grinding of Inconel 718. J Manuf Processes, 2016, 21: 124–13310.1016/j.jmapro.2015.12.004 ↗