Processing and properties of ceramic yttrium manganite sintered by different methods
Source abstract
Abstract
Intergranular and intragranular cracks that usually form during sintering of yttrium manganite (YMnO3) ceramic samples hinder the densification process of this ceramic and deteriorate its magnetic and ferroelectric properties. To overcome this problem, mechanochemically synthesized YMnO3 powder was sintered using two different processes: Conventional Sintering (CS) and Pulsed Electric Current Sintering (PECS). All samples were characterized by XRD, SEM and FESEM and their magnetic and ferroelectric properties were investigated. Apart from their phase composition, conventionally sintered ceramic samples showed cracks throughout their whole volume, reaching a maximum relative density of 85 %. However, it was found that PECS process could significantly reduce the presence of cracks within samples whose relative density reached 99.8 %.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Multiferroics and related materials · Ferroelectric and Piezoelectric Materials · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Center for Green Technologies, Institute for Multidisciplinary Research, University of Belgrade, Belgrade, Serbia
Department of Materials Science and Engineering Program, Texas A&M University, College Station, USA
Institute for Mathematics, Physics and Mechanics, Ljubljana, Slovenia
Funding
Ministry of Education, Science and Technological Development of the Republic of Serbia
References
Reference metadata was not supplied for this record.