High coercivity Sm2Fe17N3 submicron size powder prepared by polymerized-complex and reduction–diffusion process
Source abstract
Abstract
Abstract High coercivity Sm2Fe17N3 submicron size powder was synthesized by the polymerized-complex (PC), hydrogen reduction (HR) and reduction–diffusion (RD) processes. A mixture of nano size SmOx, FeOx and SmFeO3 particles was first synthesized by the polymerized-complex method, which was then reduced to α-Fe and SmOx by hydrogen. Subsequent reduction diffusion using Ca metal led to the formation of submicron size Sm2Fe17 powder with a mixture of CaO. After nitriding and rinsing, Sm2Fe17N3 powder with the average diameter of 0.69 ± 0.17 μm was obtained, which exhibited the coercivity of 2.32 T, the highest ever reported for ternary Sm2Fe17N3 anisotropic powder.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Rare-earth and actinide compounds · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Iriyama · IEEE Trans. Magn. · 1992 · 28 · 232610.1109/20.179482 ↗
2. Coey · J. Appl. Phys. · 1991 · 69 · 300710.1063/1.348614 ↗
3. Takagi · J. Magn. Magn. Mater. · 2012 · 324 · 133710.1016/j.jmmm.2011.11.035 ↗
4. Sepehri-Amin · Acta Mater. · 2015 · 99 · 29710.1016/j.actamat.2015.08.013 ↗
5. Liu · J. Alloys Compd. · 2016 · 666 · 43210.1016/j.jallcom.2015.12.227 ↗
6. Okada · J. Alloys Compd. · 2016 · 663 · 87210.1016/j.jallcom.2015.12.124 ↗
7. Imaoka · J. Alloys Compd. · 1995 · 222 · 7310.1016/0925-8388(94)04920-3 ↗
8. Kobayashi · J. Alloys Compd. · 1993 · 193 · 23510.1016/0925-8388(93)90357-S ↗
9. Wang · Solid State Commun. · 1993 · 88 · 52110.1016/0038-1098(93)90041-K ↗
10. Ding · J. Alloys Compd. · 1992 · 189 · 8310.1016/0925-8388(92)90050-J ↗
11. Ding · Appl. Phys. Lett. · 1992 · 61 · 272110.1063/1.108072 ↗
12. Ding · J. Magn. Magn. Mater. · 1992 · 115 · 21110.1016/0304-8853(92)90059-W ↗
13. Wei · J. Magn. Magn. Mater. · 1994 · 131 · 41310.1016/0304-8853(94)90285-2 ↗
14. Tada · 2012 · 48
15. Hench · Chem. Rev. · 1990 · 90 · 3310.1021/cr00099a003 ↗
16. Makita · J. Alloys Compd. · 1997 · 260 · 23610.1016/S0925-8388(97)00155-2 ↗
17. Prabhu · Scr. Mater. · 2012 · 67 · 15310.1016/j.scriptamat.2012.04.001 ↗
18. Bance · J. Appl. Phys. · 2014 · 116 · 23390310.1063/1.4904854 ↗
19. Hu · J. Magn. Magn. Mater. · 1992 · 114 · 13810.1016/0304-8853(92)90338-O ↗