journal article·2023-04

Highly stable nanoscale amorphous microstructure at steel-aluminum interface enabled by a new solid-state additive manufacturing method

M. Zhang, F.C. Liu, Z.Y. Liu, P. Xue, P. Dong, H. Zhang, L.H. Wu, D.R. Ni, Z.Y. Ma

Scripta Materialia· Volume 227
Publisher page

Abstract

In contrast to the established understanding that the interfacial microstructure of the bonded steel-aluminum (Fe-Al) structures coarsens significantly at elevated temperatures, this study shows that the special nanoscale interfacial layer of the Fe-Al bimetallic structures fabricated by a newly developed modified friction stir additive manufacturing (M-FSAM) exhibited extraordinary stability up to 500 °C. In tensile tests, the heat-treated Fe-Al samples failed within the aluminum alloys rather than along the Fe-Al interface. The heat treatment at 500 °C did not cause any observable microstructure change in the special nanoscale interfacial layer, which still consisted of a noncontinuous layer of Al-Fe-Si particles and a continuous Mg and O rich layer. The noncontinuous Al-Fe-Si particles were made of an amorphous-like microstructure and the Mg and O rich layer was comprised of an amorphous matrix interspersed with nanocrystalilne particles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Formation of nanoscale reaction layer with several crystallinities in the friction-welded 6061 Al alloy/steel joint10.1016/j.matdes.2022.110742 ↗
2. Microstructure and fracture toughness of an aluminum-steel impact weld and effect of thermal exposure10.1007/s11661-021-06269-7 ↗
3. Microstructure and mechanical property characterisation of aluminium-steel joints fabricated using ultrasonic additive manufacturing10.1080/13621718.2016.1249644 ↗
4. A comprehensive analysis of a pseudo-brittle fracture at the interface of intermetallic of η and steel in aluminum/steel joints made by FSW: microstructure and fracture behavior10.1016/j.msea.2021.141812 ↗
5. Effect of mismatch in mechanical properties on interfacial strength of aluminum alloy/steel dissimilar joints10.1016/j.msea.2020.139437 ↗
6. Formation mechanism for the nanoscale amorphous interface in pulse-welded Al/Fe bimetallic systems10.1063/1.4947465 ↗
7. A state-of-the-art review on solid-state metal joining
8. Alloy amorphization through nanoscale shear localization at Al-Fe interface
9. From thick intermetallic to nanoscale amorphous phase at Al-Fe joint interface: roles of friction stir welding conditions10.1016/j.scriptamat.2020.09.031 ↗
10. Large area friction stir additive manufacturing of intermetallic-free aluminum-steel bimetallic components through interfacial amorphization10.1016/j.jmapro.2021.11.042 ↗
11. Amorphous interfacial microstructure and high bonding strength in Al-Fe bimetallic components enabled by a large-area solid-state additive manufacturing technique10.1016/j.jmatprotec.2022.117721 ↗
12. Fatigue properties of steel to aluminum transition joints produced by explosion welding10.1016/j.ijfatigue.2020.105736 ↗
13. Modeling and analysis of thin-walled Al/steel explosion welded transition joints for shipbuilding applications10.1016/j.marstruc.2020.102843 ↗
14. Hybrid laser/arc welding of advanced high strength steel to aluminum alloy by using structural transition insert10.1016/j.matdes.2015.03.022 ↗
15. Influence of intermetallic phases and Kirkendall-porosity on the mechanical properties of joints between steel and aluminium alloys10.1016/j.msea.2011.02.057 ↗
16. Effects of heat treatments on mechanical properties of Fe/Al explosion-welded structural transition joints10.1016/j.matdes.2008.10.010 ↗
17. An isotropic glass phase in Al-Fe-Si formed by a first order transition
18. An ordered metallic glass solid solution phase that grows from the melt like a crystal10.1016/j.actamat.2013.08.063 ↗
19. Highly ordered noncrystalline metallic phase
20. Effect of annealing treatment on joint strength of aluminum/steel friction stir lap weld10.1016/j.matdes.2012.08.028 ↗
21. Effects of post-weld heat treatment on dissimilar metal joint between aluminum alloy and stainless steel10.1016/j.msea.2012.04.110 ↗
22. Determining the three-dimensional atomic structure of an amorphous solid10.1038/s41586-021-03354-0 ↗
23. Formation of Al-Fe-Si glass that grows from the melt through a first-order transition10.1016/j.jallcom.2012.01.056 ↗
24. Phase transformation during annealing of rapidly solidified Al- rich Al-Fe-Si alloys10.1007/BF02647715 ↗
25. Formation and crystallization of Al-Fe-Si amorphous alloys10.1007/BF00551989 ↗
26. Amorphization of rapidly quenched quasicrystalline Al-transition metal alloys by the addition of Si10.1557/JMR.1986.0415 ↗
27. Heterogeneous nucleation mechanism in Al-Fe-Si amorphous alloys10.1016/S0921-5093(00)01491-X ↗
28. New amorphous alloys in Al-Si-Fe-TM (TM = Cr, Mn, V) systems and their crystallization behavior10.1023/A:1026457914226 ↗