journal article·2006-02

Bulk ultrafine binderless WC prepared by spark plasma sintering

B HUANG, L CHEN, S BAI

Scripta Materialia· Volume 54· Issue 3
Publisher page

Abstract

Abstract Pure WC powder of about 200 nm in diameter was sintered by the spark plasma sintering process without the addition of any binder phase. The initial ultrafine particle size was basically maintained after sintering. The binderless WC sintered at 1773 K for 240 s showed almost full densification and exhibited excellent mechanical properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.