journal article·2016-03Open access

In-situ transmission electron microscopy study of surface oxidation for Ni–10Cr and Ni–20Cr alloys

Langli Luo, Lianfeng Zou, Daniel K. Schreiber, Donald R. Baer, Stephen M. Bruemmer, Guangwen Zhou, Chong-Min Wang

Scripta Materialia· Volume 114

Abstract

Abstract The early-stage oxidation of Ni (001) thin films alloyed with 10 or 20 at.% Cr at 700 °C has been directly visualized using in-situ TEM. Independent of Cr concentration, the oxidation initiates via nucleation of surface NiO islands and subsurface Cr2O3. The NiO grows and transitions into a continuous film, followed by the nucleation and growth of NiCr2O4 islands. For Ni–20 at.% Cr, a continuous Cr2O3 was developed, but not for Ni–10 at.% Cr. NiO whiskers are observed to preferentially nucleate/grow from the NiCr2O4 islands through a short-circuit diffusion of Ni along the NiCr2O4 interfaces in Ni–10 at.% Cr.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Douglass · Corros. Sci. · 1968 · 8 · 66510.1016/S0010-938X(68)80101-5 ↗
2. Chattopadhyay · J. Electrochem. Soc. · 1970 · 117 · 116310.1149/1.2407761 ↗
3. Wood · Corros. Sci. · 1970 · 10 · 47110.1016/S0010-938X(70)80032-4 ↗
4. Dangsheng · Wear · 2001 · 251 · 109410.1016/S0043-1648(01)00803-1 ↗
5. Bangala · AlChE J. · 1998 · 44 · 92710.1002/aic.690440418 ↗
6. Liu · J. Am. Chem. Soc. · 2009 · 131 · 1667810.1021/ja9079308 ↗
7. Besenbacher · Science · 1998 · 279 · 191310.1126/science.279.5358.1913 ↗
8. Atkinson · Oxid. Met. · 1985 · 24 · 17710.1007/BF00664231 ↗
9. Baer · Metall. Trans. A · 1980 · 11 · 197310.1007/BF02655116 ↗
10. Baer · Appl. Surf. Sci. · 1981 · 7 · 6910.1016/0378-5963(81)90061-1 ↗
11. Yang · Appl. Phys. Lett. · 1997 · 70
12. Flower · Corros. Sci. · 1977 · 17 · 25310.1016/0010-938X(77)90050-6 ↗
13. Marikar · Ultramicroscopy · 1989 · 29 · 24710.1016/0304-3991(89)90252-0 ↗
14. Yang · Appl. Phys. Lett. · 1998 · 73 · 284110.1063/1.122608 ↗
15. Eastman · Appl. Phys. Lett. · 2005 · 87 · 05191410.1063/1.2005396 ↗
16. Zhou · Phys. Rev. Lett. · 2005 · 94 · 24610110.1103/PhysRevLett.94.246101 ↗
17. Luo · Phys. Rev. B · 2011 · 83 · 15541810.1103/PhysRevB.83.155418 ↗
18. Zhou · Phys. Rev. Lett. · 2012 · 109 · 23550210.1103/PhysRevLett.109.235502 ↗
19. Luo · Appl. Phys. Lett. · 2014 · 104 · 12160110.1063/1.4870085 ↗
20. Chattopadhyay · Oxid. Met. · 1970 · 2 · 37310.1007/BF00604477 ↗
21. Calvarin · Oxid. Met. · 2000 · 53 · 2510.1023/A:1004578513020 ↗
22. Gignac · Microsc. Microanal. · 2011 · 17 · 88910.1017/S1431927611011974 ↗
23. Schreiber · Microsc. Microanal. · 2012 · 18 · 141010.1017/S1431927612013517 ↗