Fatigue damage in bulk metallic glass II: Experiments

P HESS, B MENZEL, R DAUSKARDT

Scripta Materialia· Volume 54· Issue 3
Publisher page

Abstract

Abstract Cyclic fatigue was investigated in metallic glasses using fracture mechanics-based crack-growth and stress-life experiments. Steady-state crack growth in a Zr-based bulk metallic glass occurred with a Paris law exponent of ∼1.5. Growing planar fatigue cracks were often noted to destabilize into a wavy crack front geometry, and the conditions determining the stability of these cracks are analyzed. Transient crack-growth rates were measured during variable-amplitude fatigue. Stress-life experiments showed low endurance limits. Fatigue damage initiated at an angle to the applied load, but changed direction at a critical length and grew as mode I cracks. However, the initiation stage of fatigue damage was very short, and almost the entire fatigue life was spent in the crack-growth stage.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.