journal article·2017-10

Effect of cristobalite formation on the delamination resistance of an oxide/Si/(SiC/SiC) environmental barrier coating system after cyclic high temperature thermal exposure

Yutaro Arai, Yuto Aoki, Yutaka Kagawa

Scripta Materialia· Volume 139
Publisher page

Abstract

Abstract Delamination toughness of a mullite/Si/(SiC/SiC) environmental barrier coating (EBC) system has been measured using a shear-loading test. The EBC system is initially heated to a temperature of 1470 °C (above the melting point of Si (1414 °C)), and then repeated thermal exposure is carried out at a temperature 1320 °C (below the melting point of Si) for 2 h/cycle. Change of the delamination toughness with heat exposure is successfully obtained using the shear-loading test. Formation of cristobalite and transformation from α ↔ β during thermal cycling cause an increase of crack density in the Si bond coat layer and a resulting reduction in delamination toughness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Eaton · J. Eur. Ceram. Soc. · 2002 · 22 · 274110.1016/S0955-2219(02)00141-3 ↗
2. More · J. Am. Ceram. Soc. · 2003 · 86 · 127210.1111/j.1151-2916.2003.tb03463.x ↗
3. Spitsberg · Int. J. Appl. Ceram. Technol. · 2004 · 1 · 29110.1111/j.1744-7402.2004.tb00181.x ↗
4. Lee · J. Am. Ceram. Soc. · 2003 · 86 · 129910.1111/j.1151-2916.2003.tb03466.x ↗
5. Lee · J. Eur. Ceram. Soc. · 2005 · 25 · 170510.1016/j.jeurceramsoc.2004.12.013 ↗
6. Ramasamy · Surf. Coat. Technol. · 2011 · 205 · 357810.1016/j.surfcoat.2010.12.031 ↗
7. Cojocaru · Spray Technol. · 2010 · 20 · 9210.1007/s11666-010-9599-4 ↗
8. Dicarlo · 2015 · 217
9. Lee · 2015 · 430
10. Stolzenburg · Acta Mater. · 2016 · 105 · 18910.1016/j.actamat.2015.12.016 ↗
11. Richards · J. Am. Ceram. Soc. · 2015 · 98 · 406610.1111/jace.13792 ↗
12. Richards · Acta Mater. · 2016 · 106 · 110.1016/j.actamat.2015.12.053 ↗
13. Okada · J. Appl. Phys. · 1984 · 56 · 31410.1063/1.333965 ↗
14. Kuribara · 2014
15. Aoki · Surf. Coat. Technol. · 2017 · 321 · 21310.1016/j.surfcoat.2017.03.073 ↗
16. Takeda · J. Am. Ceram. Soc. · 1999 · 82 · 157910.1111/j.1151-2916.1999.tb01960.x ↗
17. Caradarelli · 2000 · 339
18. Bates · J. Chem. Phys. · 1972 · 57 · 404210.1063/1.1678878 ↗
19. Arai · 2017
20. Nakashima · Phys. Status Solidi A · 1997 · 162 · 3910.1002/1521-396X(199707)162:1<39::AID-PSSA39>3.0.CO;2-L ↗
21. Anastassakis · Solid State Commun. · 1970 · 8 · 13310.1016/0038-1098(70)90588-0 ↗
22. Hridenreich · 2015 · 147
23. Schneider · 2005 · 156
24. Y. Arai and Y. Kagawa, Residual stress in Si bond coat layer after high temperature heat exposure, (to be submitted).
25. Hutchinson · J. Am. Ceram. Soc. · 2011 · 94 · s8510.1111/j.1551-2916.2011.04499.x ↗
26. Messmer · J. Appl. Phys. · 1981 · 52 · 462310.1063/1.329342 ↗