Peculiar temperature dependence of hydrogen-enhanced fatigue crack growth of low-carbon steel in gaseous hydrogen
Source abstract
Abstract
Abstract The peculiar temperature dependence of hydrogen-enhanced fatigue crack growth (HEFCG) of low-carbon steel in hydrogen gas was successfully interpreted in terms of ‘trap-site occupancy’ of hydrogen. HEFCG decreased with increasing temperature in hydrogen gas at 0.7 MPa and 298 to 423 K due to lower occupancy of trap sites at higher temperatures. In hydrogen gas at 90 MPa, HEFCG was insensitive to the temperature because most of the trap sites were occupied by hydrogen, regardless of the temperature. Trap sites with a binding energy of 47 kJ/mol, corresponding approximately to the dislocation core, dominated the temperature dependence of HEFCG.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Engineering Diagnostics and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Williams · Metall. Mater. Trans. B Process Metall. Mater. Process. Sci. · 1970 · 1 · 63
2. Smith · Met. Sci. · 1979 · 13 · 42910.1179/msc.1979.13.7.429 ↗
3. Marrow · Acta Metall. · 1992 · 40 · 205910.1016/0956-7151(92)90192-H ↗
4. Landes · Int. J. Fract. · 1973 · 9 · 27710.1007/BF00049196 ↗
5. Saito · Trans. Iron Steel Inst. Jpn. · 1984 · 24 · 105510.2355/isijinternational1966.24.1055 ↗
6. Gerberich · Metall. Trans. A. · 1988 · 19 · 131910.1007/BF02662593 ↗
7. Arioka · Corrosion (Houston, TX, U. S.) · 2007 · 63 · 111410.5006/1.3278329 ↗
8. Yoshikawa · Trans. Jpn. Soc. Mech. Eng. A · 2010 · 76 · 90810.1299/kikaia.76.908 ↗
9. Yamabe · J. Press. Vessel. Technol. · 2016 · 13810.1115/1.4030086 ↗
10. Matsunaga · Philos. Trans. R. Soc. A · 2017 · 375 · 2016041210.1098/rsta.2016.0412 ↗
11. Itoga · 2014
12. ASTM E647-15e1 · 2010
13. Laird · Philos. Mag. · 1962 · 7 · 84710.1080/14786436208212674 ↗
14. Bichler · 1999 · 211
15. Matsuoka · Eng. Fract. Mech. · 2016 · 153 · 10310.1016/j.engfracmech.2015.12.023 ↗
16. Matsuoka · Int. J. Fract. · 2011 · 168 · 10110.1007/s10704-010-9560-z ↗
17. Oriani · Acta Metall. · 1970 · 18 · 14710.1016/0001-6160(70)90078-7 ↗
18. Quick · Acta Metall. · 1978 · 26 · 90310.1016/0001-6160(78)90041-X ↗
19. San Marchi · Int. J. Hydrog. Energy · 2007 · 32 · 10010.1016/j.ijhydene.2006.05.008 ↗
20. Taketomi · Acta Mater. · 2008 · 56 · 376110.1016/j.actamat.2008.04.011 ↗
21. Matsumoto · Int. J. Hydrog. Energy · 2009 · 34 · 957610.1016/j.ijhydene.2009.09.052 ↗
22. Ferreira · Acta Mater. · 1998 · 46 · 174910.1016/S1359-6454(97)00349-2 ↗
23. Tabata · Scr. Metall. · 1983 · 17 · 94710.1016/0036-9748(83)90268-5 ↗
24. Birnbaum · Mater. Sci. Eng. A · 1994 · 176 · 19110.1016/0921-5093(94)90975-X ↗
25. Wang · Acta Mater. · 2018 · 144 · 16410.1016/j.actamat.2017.10.034 ↗
26. Ogawa · Scr. Mater. · 2017 · 140 · 1310.1016/j.scriptamat.2017.06.037 ↗
27. Tien · Metall. Trans. A. · 1976 · 7 · 82110.1007/BF02644079 ↗
28. Dadfarnia · J. Mech. Phys. Solids · 2015 · 78 · 51110.1016/j.jmps.2015.03.002 ↗