Ultra-fine microstructure and exceptional low coercivity developed in a high-Bs Fe-Si-B-P alloy by co-alloying Ni, Mo, and Cu
Source abstract
Abstract
Designing soft magnetic alloys with high saturation magnetic induction ( B s) is of great importance for improving the power density of electric and electronic devices. For high- B s nanocrystalline alloys, the main problem is the grain coarsening effect induced by high Fe content (>80 at.%), which deteriorates the soft magnetic properties. In present work, we designed new Fe-based nanocrystalline alloys by microalloying a Fe-Si-B-P alloy. The co-alloying of Ni, Mo, and Cu effectively refines the microstructure of nanocrystalline alloys from 28.5 nm to 13.1 nm and increased the stability of soft magnetic properties. Even though there are 28-nm-large surface crystallites in the amorphous precursors, an exceptional low coercivity of 1–2 A/m with a high B s of 1.81 T was developed after nanocrystallization. These excellent magnetic properties could be maintained within a wide annealing temperature window of 50 K and an annealing time window up to 600 s for high heating rate annealing.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · High Entropy Alloys Studies · Magnetic properties of thin films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Soft magnetic materials for a sustainable and electrified world10.1126/science.aao0195 ↗
2. Modern soft magnets: amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
3. Fe-based bulk metallic glasses: glass formation, fabrication, properties, and applications10.1016/j.pmatsci.2019.01.003 ↗
4. High Bs of FePBCCu nanocrystalline alloys with excellent soft-magnetic properties10.1016/j.jnoncrysol.2019.119800 ↗
5. Microstructure and soft magnetic properties of FeCoPCCu nanocrystalline alloys10.1016/j.jmst.2019.03.030 ↗
6. Composition design for Fe-based soft magnetic amorphous and nanocrystalline alloys with high Fe content10.1016/j.matdes.2020.108511 ↗
7. Formation and crystallization behavior of Fe-based amorphous precursors with pre-existing alpha-Fe nanoparticles - Structure and magnetic properties of high-Cu-content Fe-Si-B-Cu-Nb nanocrystalline alloys10.1016/j.jmst.2020.05.049 ↗
8. Effects of minor precipitation of large size crystals on magnetic properties of Fe-Co-Si-B-P-Cu alloy10.1016/j.jallcom.2017.03.193 ↗
9. Exceptionally high saturation magnetic flux density and ultralow coercivity via an amorphous-nanocrystalline transitional microstructure in an FeCo-based alloy
10. Grain structure and magnetism of nanocrystalline ferromagnets10.1109/20.42292 ↗
11. Soft magnetic nanocrystalline materials10.1016/0956-716X(95)00397-E ↗
12. Random magnetocrystalline anisotropy in two-phase nanocrystalline systems10.1103/PhysRevB.58.2730 ↗
13. On the role of Cu and Nb in the formation of nanocrystals in amorphous Fe73.5Nb3Cu1Si13.5B910.1063/1.110923 ↗
14. On the formation of nanocrystals in the soft magnetic alloys Fe73.5Nb3Cu1Si13.5B910.1016/S1359-6454(97)00436-9 ↗
15. Cu clustering and Si partitioning in the early crystallization stage of an Fe73.5Si13.5B9Nb3Cu1 amorphous alloy10.1016/S1359-6454(98)00392-9 ↗
16. Competition driven nanocrystallization in high Bs and low core loss Fe-Si-B-P-Cu soft magnetic alloys10.1016/j.scriptamat.2014.08.023 ↗
17. Copper-free nanocrystalline soft magnetic materials with high saturation magnetization comparable to that of Si steel10.1063/1.4973772 ↗
18. Effect of heating rate during primary crystallization on soft magnetic properties of melt-spun Fe-B alloys10.1016/j.scriptamat.2017.01.030 ↗
19. Core loss of ultra-rapidly annealed Fe-rich nanocrystalline soft magnetic alloys10.1016/j.jmmm.2018.12.053 ↗
20. Nanocrystalline soft magnetic materials produced by continuous ultra-rapid annealing (CURA)10.1063/9.0000274 ↗
21. Influence of thermal history on the crystallization behavior of high-Bs Fe-based amorphous alloys10.1007/s11433-022-2079-1 ↗
22. Nanostructural formation kinetics in an Fe86B14 soft magnetic alloy investigated by in situ transport measurements under isothermal conditions
23. K. Onodera, K. Suzuki, R. Parsons, B. Zang, Method for producing soft magnetic material, PCT/JP2017/028128.
24. Nano-crystallisation and magnetic softening in Fe-B binary alloys induced by ultra-rapid heating10.1088/1361-6463/aadad6 ↗
25. A study on the role of Ni content on structure and properties of Fe-Ni-Si-B-P-Cu nanocrystalline alloys10.1016/j.jallcom.2019.152784 ↗
26. Dramatic grain refinement and magnetic softening induced by Ni addition in Fe-B based nanocrystalline soft magnetic alloys10.1016/j.scriptamat.2020.02.020 ↗
27. Role of Mo addition on structure and magnetic properties of Fe85Si2B8P4Cu1 nanocrystalline alloy10.1016/j.jnoncrysol.2017.12.003 ↗
28. Heterostructured crystallization mechanism and its effect on enlarging the processing window of Fe-based nanocrystalline alloys10.1016/j.jmst.2020.08.020 ↗
29. Direct synthesis of Fe-Si-B-C-Cu nanocrystalline alloys with superior soft magnetic properties and ductile by melt-spinning10.1016/j.jmst.2021.08.055 ↗
30. Effect of Si/B ratio on magnetic properties and microstructure of FeSiBNbCuAl nanocrystalline alloys10.1016/j.jnoncrysol.2021.120839 ↗
31. Observation of Cu nanometer scale clusters formed in Fe85Si2B8P4Cu1 nanocrystalline soft magnetic alloy by a spherical aberration-corrected TEM/STEM10.1080/09500839.2015.1052584 ↗
32. Inheritance from glass to liquid: beta relaxation depresses the nucleation of crystals10.1016/j.actamat.2019.12.002 ↗
33. Existence of multiple critical cooling rates with generate different types of monolithic metallic glasses10.1038/s41467-018-07930-3 ↗
34. Supercluster-coupled crystal growth in metallic glass forming liquids10.1038/s41467-019-08898-4 ↗