Comparing the intergranular oxidation of Ni-Cr and Ni-Al model alloys in 480 °C hydrogenated steam
Source abstract
Abstract
The intergranular oxidation of binary Ni-xAl ( x = 4, 7 at.%) and Ni-yCr ( y = 11, 15 at.%) model alloys was studied in a 480 °C hydrogenated steam environment. It was observed that the intergranular oxidation susceptibility in Ni-Al and Ni-Cr alloys is different. In Ni-Al alloys, HAGBs are very susceptible to intergranular oxidation, while low energy grain boundaries behave similar to bulk material. In Ni-Cr alloys, LAGBs and CSLBs are susceptible to intergranular oxidation, while HAGBs are protected by an external oxide. The structure of the intergranular oxide was also different between Ni-Cr and Ni-Al alloys; the intergranular oxide formed in Ni-Al alloys was sharper and penetrated to greater depth compared with Ni- Cr alloys. Comparisons are made to previous testing of alloy 600 (Ni-16Cr-Fe) in similar environments, highlighting the potential effect of residual Al and Ti on the intergranular oxidation of the alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Internal oxidation of Ag-In alloys: stress relief and the influence of imposed strain10.1007/BF00664274 ↗
2. A review of oxidation phenomena in Ni alloys exposed to hydrogenated steam below 500°C10.5006/1957 ↗
3. Internal oxidation of Ag-xIn alloys at low homologous temperature10.1016/j.corsci.2020.108869 ↗
4. Grain boundary selective oxidation and intergranular stress corrosion crack growth of high-purity nickel binary alloys in high-temperature hydrogenated water10.1016/j.corsci.2017.11.024 ↗
5. A mechanistic study of SCC in Alloy 600 through high-resolution characterization10.1016/j.corsci.2018.01.004 ↗
6. Alloy oxidation studies related to PWSCC
7. Some possible mechanisms of intergranular stress corrosion cracking of alloy 600 in PWR primary water
8. The role of grain boundary misorientation in intergranular cracking of Ni-16Cr-9Fe in 360°C argon and high purity water10.1007/BF02665051 ↗
9. The effect of temperature on the preferential intergranular oxidation susceptibility of alloy 60010.1007/s11661-018-4491-9 ↗
10. The high-temperature internal oxidation and intergranular oxidation of nickel-chromium alloys10.1016/0010-938X(83)90056-2 ↗
11. Effect of temperature on the preferential intergranular oxidation susceptibility of thermally-treated Alloy 60010.1016/j.corsci.2022.110565 ↗
12. TEM investigations of intergranular stress corrosion cracking in austenitic alloys in PWR environmental conditions10.1179/mht.2003.066 ↗
13. Characterization of initial intergranular oxidation processes in alloy 600 at a sub-nanometer scale10.1016/j.corsci.2018.01.020 ↗
14. The effect of grain boundary structure on the intergranular degradation behavior of solution annealed alloy 690 in high temperature, hydrogenated water10.1016/j.actamat.2019.10.041 ↗
15. The intergranular oxidation behavior of low-angle grain boundary of alloy 600 in simulated pressurized water reactor primary water10.1016/j.actamat.2021.117533 ↗
16. Development of preferential intergranular oxides in nickel-aluminum alloys at high temperatures10.1007/BF00662032 ↗
17. Directly correlated transmission electron microscopy and atom probe tomography of grain boundary oxidation in a Ni–Al binary alloy exposed to high-temperature water10.1016/j.scriptamat.2013.06.008 ↗
18. Grain boundary depletion and migration during selective oxidation of Cr in a Ni–5Cr binary alloy exposed to high-temperature hydrogenated water10.1016/j.scriptamat.2014.06.022 ↗
19. The effect of residual stress on the Preferential Intergranular Oxidation of Alloy 60010.1016/j.corsci.2016.05.022 ↗
20. Grain boundary misorientation effects on creep and cracking in Ni-based alloys10.1007/s11837-998-0249-y ↗
21. Priester · 2013
22. Structure-dependent intergranular oxidation in Ni–Fe polycrystalline alloy10.1016/S1359-6454(99)00007-5 ↗
23. Influence of grain boundary character distribution on sensitization and intergranular corrosion of alloy 60010.1016/0956-716X(95)00420-Z ↗
24. Applications for Grain Boundary Engineered Materials10.1007/s11837-998-0248-z ↗
25. Grain boundary oxidation behavior of Ni-15Cr alloy in high temperature carbon dioxide10.1016/j.scriptamat.2022.114935 ↗
26. Internal oxidation of Alloy 600 exposed to hydrogenated steam and the beneficial effects of thermal treatment10.1016/j.corsci.2014.04.041 ↗
27. Y. Ghaffari, K. Daub, and S.Y. Persaud, "Oxidation of Ni-Cr-Al model alloys in 480 ˚C hydrogenated steam," (manuscript under preparation).
28. The structure of high-angle grain boundaries10.1016/0001-6160(66)90168-4 ↗
29. Young · 2008
30. The influence of alloying elements on the development and maintenance of protective scales10.1007/BF01046725 ↗
31. Structural evolution of a Ni alloy surface during high-temperature oxidation10.1007/s11085-017-9821-6 ↗
32. Penetration of oxygen along grain boundaries during oxidation of alloys and intermetallics10.1007/BF01050802 ↗
33. Advanced microstructural characterization of the intergranular oxidation of Alloy 60010.1016/j.corsci.2015.08.010 ↗
34. Replicating PWR primary water conditions in low pressure H2-steam environment to study alloy 600 oxidation processes10.1149/2.0081902jes ↗
35. On the role of intergranular nanocavities in long-term stress corrosion cracking of Alloy 69010.1016/j.actamat.2021.117453 ↗
36. Stress corrosion crack initiation in Alloy 690 in high temperature water10.1016/j.cossms.2018.02.001 ↗
37. Ab initio modeling of bulk and intragranular diffusion in Ni alloys10.1021/acs.jpclett.5b00177 ↗
38. High resolution analysis of oxidation in Ni-Fe-Cr alloys after exposure to 315°C deaerated water with added hydrogen10.1016/j.corsci.2016.02.009 ↗