Retrogression and reaging (RRA) treatment is a distinctive approach to counteract hydrogen embrittlement in 7xxx Al alloys without compromising strength. However, the mechanistic understanding of RRA has long centered around grain-boundary-related phenomena, while the roles of grain-interior microstructures in hydrogen embrittlement have remained unclear. Here, we demonstrate the beneficial effect of RRA in reducing transgranular cracks in a specially selected high-Zn alloy that exhibits fully quasi-cleavage cracking, thereby enabling the precise decoupling of grain-interior and grain-boundary mechanisms. Using synchrotron radiation 3D observations, we identify a significant delay in the initiation of transgranular cracks in RRA-treated specimens as compared to those in the peak-aged condition. Atomic-resolution electron microscopy observations confirm the grain-interior partial transformation from the coherent η’ phase to the semi-coherent η phase. It is proposed that the increased fraction of semi-coherent η/Al interfaces reduces hydrogen coverage at coherent interfaces, thereby suppressing transgranular hydrogen-induced debonding on the slip planes.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Environment-induced cracking of high-strength Al-Zn-Mg-Cu aluminum alloys: past, present, and future10.5006/4149 ↗
2. Comparison of 5th-generation fighters: evaluation of trends in military aviation
3. An overview of high-performance aircraft structural Al alloy-AA708510.1007/s40195-015-0275-z ↗
4. Stress corrosion cracking in Al-Zn-Mg-Cu aluminum alloys in saline environments10.1007/s11661-012-1528-3 ↗
5. The postulated mechanisms for stress corrosion cracking of aluminum alloys: a review of the literature 1980-198910.5006/1.3585235 ↗
6. Reversion and re-aging of a peak aged Al-Zn-Mg-Cu alloy10.1016/j.scriptamat.2020.07.049 ↗
7. Evolution of precipitate microstructures during the retrogression and re-ageing heat treatment of an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2010.05.017 ↗
8. A phase field formulation for dissolution-driven stress corrosion cracking10.1016/j.jmps.2020.104254 ↗
9. Phase-field simulations opening new horizons in corrosion research
10. Resistance of CoCrFeMnNi high-entropy alloy to gaseous hydrogen embrittlement10.1016/j.scriptamat.2017.03.029 ↗
11. Comparative study of hydrogen embrittlement in stable and metastable high-entropy alloys10.1016/j.scriptamat.2018.03.003 ↗
12. Revisiting the precipitation mechanisms of Guinier-Preston zones, η′, and η precipitates in Al-Zn-Mg alloys10.1016/j.actamat.2024.119789 ↗
13. GP-zones in Al–Zn–Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
14. The nucleation of precipitates: the system Al-Zn-Mg10.1016/0001-6160(65)90067-2 ↗
15. Cina · 1974
16. Retrogression and reaging and the role of dislocations in the stress corrosion of 7000-type aluminum alloys10.1007/BF02650294 ↗
17. Effect of retrogression and reaging treatments on the microstructure of Ai-7075-T65110.1007/BF02657792 ↗
18. Influence of retrogression and reaging treatments on the strength and stress corrosion resistance of aluminium alloy 7075-T610.1016/0025-5416(88)90512-5 ↗
19. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
20. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interfaces of nanoprecipitates in martensitic steels10.1038/s41467-022-31665-x ↗
21. Enhanced hydrogen embrittlement of steel by the premature hydrogen dissociation with the increasing inert gas pressure in hydrogen-containing mixtures10.1016/j.actamat.2023.119279 ↗
22. Hydrogen-accelerated spontaneous microcracking in high-strength aluminium alloys10.1038/s41598-020-58834-6 ↗
23. First-principles study of hydrogen segregation at the MgZn2 precipitate in Al-Mg-Zn alloys10.1016/j.commatsci.2018.03.009 ↗
24. The evolution of precipitates in an Al–Zn–Mg alloy10.1016/j.jmrt.2023.02.144 ↗
25. Atomic structure of hardening precipitates in an Al–Mg–Zn–Cu alloy determined by HAADF-STEM and first-principles calculations: relation to η-MgZn 210.1007/s10853-013-7158-3 ↗
26. Switching nanoprecipitates to resist hydrogen embrittlement in high-strength aluminum alloys10.1038/s41467-022-34628-4 ↗
27. Mechanisms of hydrogen embrittlement in high-strength aluminum alloys containing coherent or incoherent dispersoids10.1016/j.corsci.2021.109895 ↗
28. Hydrogen diffusion and trapping in a low copper 7xxx aluminium alloy investigated by scanning Kelvin probe force microscopy10.1016/j.msea.2017.08.119 ↗
29. Revisiting stress-corrosion cracking and hydrogen embrittlement in 7xxx-Al alloys at the near-atomic-scale10.1038/s41467-022-31964-3 ↗
30. Role of grain-boundary precipitates and solute-depleted zone on the intergranular corrosion of aluminum alloy 715010.5006/1.3287699 ↗
31. Improvement of fracture toughness in 7475 aluminum alloy by the RRA (retrogression and re-aging) process10.2320/matertrans1989.30.601 ↗
32. In-situ 3D observation of hydrogen-assisted particle damage behavior in 7075 Al alloy by synchrotron X-ray tomography10.1016/j.actamat.2022.117658 ↗
33. Influence of hydrogen on strain localization and fracture behavior in AlZnMgCu aluminum alloys10.1016/j.actamat.2018.08.024 ↗
34. Toda · 2021
35. Multimodal assessment of mechanically induced transformation in metastable multi-phase steel using X-ray nano-tomography and pencil-beam diffraction tomography10.1016/j.actamat.2022.117956 ↗
36. Ultrathin specimen preparation by a low-energy Ar-ion milling method10.1093/jmicro/dfs073 ↗
37. Inelastic mean free path measurement by STEM-EELS technique using needle-shaped specimen10.1016/j.ultramic.2020.112955 ↗
38. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
39. Stress corrosion cracking induced by the combination of external and internal hydrogen in Al-Zn-Mg-Cu alloy10.1016/j.scriptamat.2023.115804 ↗
40. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
41. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
42. Improving the hydrogen embrittlement resistance by straining the ferrite /cementite interfaces10.1016/j.actamat.2024.119850 ↗
43. Strain gradient plasticity-based modeling of hydrogen environment assisted cracking10.1016/j.actamat.2016.07.022 ↗
44. Enhanced hydrogen embrittlement of low-carbon steel to natural gas/hydrogen mixtures10.1016/j.scriptamat.2020.08.011 ↗
45. Hydrogen-trapping energy in screw and edge dislocations in aluminum: first-principles calculations10.2320/matertrans.MT-M2020375 ↗
46. Hydrogen embrittlement of aluminum: the crucial role of vacancies10.1103/PhysRevLett.94.155501 ↗
47. Hydrogenated vacancies lock dislocations in aluminium10.1038/ncomms13341 ↗
48. Effect of hydrogen environment on the separation of Fe grain boundaries10.1016/j.actamat.2016.01.067 ↗
49. Atomistic study of hydrogen embrittlement of grain boundaries in nickel: II. Decohesion10.1088/1361-651X/aa87a6 ↗
50. First-principles study on the grain boundary embrittlement of metals by solute segregation: Part II. Metal (Fe, Al, Cu)-hydrogen (H) systems10.1007/s11661-010-0380-6 ↗