Thermally induced planar defect formation in sputtered V1-xMoxB2-Δ films
Source abstract
Abstract
This work reports on various thermally induced planar defects formed in ternary V 1-xMo xB 2-Δ coatings with different influence on mechanical properties. V 0.58Mo 0.42B 1.9 and V 0.37Mo 0.63B 1.2 films were prepared by magnetron sputtering and annealed in vacuum up to 1300 °C. Depending on the stoichiometry, different types of planar defects were identified by scanning transmission electron microscopy (STEM). In the slightly understoichiometric V 0.58Mo 0.42B 1.9 system, anti-phase boundary defects (APB) were observed, which was accompanied by chemical separation of V and Mo. Accumulation of these defects led to formation of MoB-Cmcm orthorhombic phase in otherwise hexagonal VB 2-P6/mmm structure, with no apparent effect on mechanical properties. On the other hand, in case of the highly understoichiometric V 0.37Mo 0.63B 1.2 coating, no chemical separation was observed. Here, annealing resulted in crystallization from amorphous state into orthorhombic Cmcm phase with high density of twin lamellae, which was accompanied by a significant hardening.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Borides in thin film technology10.1006/jssc.1997.7456 ↗
2. Evaluation of TiB2 coatings in sliding contact against aluminium10.1016/S0257-8972(01)01361-5 ↗
3. Tribological properties of selected PVD coatings when slid against ductile materials10.1016/S0043-1648(02)00011-X ↗
4. Tribological behaviour of pulsed magnetron sputtered CrB2 coatings examined by reciprocating sliding wear testing against aluminium alloy and steel10.1016/j.surfcoat.2007.06.057 ↗
5. Evaluation of TiB2 coatings in cold forming of aluminium10.1179/1743294412Y.0000000017 ↗
6. Self-organized nanocolumnar structure in superhard TiB2 thin films10.1063/1.1887824 ↗
7. Stoichiometry, structure and mechanical properties of co-sputtered Ti 1-x Ta x B 2±Δ coatings10.1016/j.surfcoat.2019.04.017 ↗
8. Structure evolution and mechanical properties of hard tantalum diboride films10.1116/6.0000155 ↗
9. Hard and wear resistant VB2 coatings deposited by pulsed DC magnetron sputtering10.1016/j.vacuum.2016.09.014 ↗
10. Revisiting the origins of super-hardness in TiB2+z thin films – Impact of growth conditions and anisotropy10.1016/j.surfcoat.2022.128806 ↗
11. Synthesis and characterization of MoB2−x thin films grown by nonreactive DC magnetron sputtering10.1116/1.4948234 ↗
12. Synthesis and characterization of (Ti1-xAlx)B2+Δ thin films from combinatorial magnetron sputtering10.1016/j.tsf.2018.10.042 ↗
13. Age hardening in (Ti1 − xAlx)B2 + Δ thin films10.1016/j.scriptamat.2016.09.021 ↗
14. Solid solution hardening of vacancy stabilized TixW1−xB210.1016/j.actamat.2015.08.048 ↗
15. Improved oxidation properties from a reduced B content in sputter-deposited TiBx thin films10.1016/j.surfcoat.2021.127353 ↗
16. Multifunctional ZrB2-rich Zr1-xCrxBy thin films with enhanced mechanical, oxidation, and corrosion properties10.1016/j.vacuum.2020.109990 ↗
17. Strategy for simultaneously increasing both hardness and toughness in ZrB 2 -rich Zr 1−x Ta x B y thin films10.1116/1.5093170 ↗
18. Effect of reflected Ar neutrals on tantalum diboride coatings prepared by direct current magnetron sputtering10.1016/j.surfcoat.2021.127463 ↗
19. On the nature of planar defects in transition metal diboride line compounds10.1016/j.mtla.2022.101478 ↗
20. Where is the unpaired transition metal in substoichiometric diboride line compounds?10.1016/j.actamat.2020.116510 ↗
21. Impact of vacancies on structure, stability and properties of hexagonal transition metal diborides, MB2 (M = Sc, Y, Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, Mn, and Fe)10.1016/j.mtla.2022.101629 ↗
22. Review of transition-metal diboride thin films10.1016/j.vacuum.2021.110567 ↗
23. Structure, stability, and mechanical properties of boron-rich Mo-B phases: a computational study10.1021/acs.jpclett.0c00242 ↗
24. Structure and phase evolution of Cr-Al-N coatings during annealing10.1016/j.surfcoat.2008.04.075 ↗
25. Thermally induced age hardening in tough Ta-Al-N coatings via spinodal decomposition10.1063/1.4981534 ↗
26. Thermal stability and structural evolution of quaternary Ti-Ta-B-N coatings10.1016/j.surfcoat.2014.10.009 ↗
27. Crystallographic tool box (CrysTBox): automated tools for transmission electron microscopists and crystallographers10.1107/S1600576715017252 ↗
28. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
29. Indentation hardness measurements at macro-, micro-, and nanoscale: a critical overview10.1007/s11249-016-0805-5 ↗
30. Influence of boron vacancies on phase stability, bonding and structure of MB2 (M = Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W) with AlB2 type structure10.1088/0953-8984/27/43/435702 ↗
31. Ab initio inspired design of ternary boride thin films10.1038/s41598-018-27426-w ↗
32. Synthesis and characterisation of nanocomposite Mo-Fe-B thin films deposited by magnetron sputtering10.3390/ma14071739 ↗
33. Structural stability and the alloying effect of TiB polymorphs in TiAl alloys10.1016/j.intermet.2017.07.002 ↗
34. Deformation induced twinning and phase transition in an interstitial intermetallic compound niobium boride10.1016/j.actamat.2018.12.011 ↗
35. The evolution of microstructure in a laser clad TiB-Ti composite coating10.1016/S1359-6454(02)00475-5 ↗
36. Synthesis and characterization of CrB2 thin films grown by DC magnetron sputtering10.1016/j.scriptamat.2021.113915 ↗
37. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
38. The cleavage strength of polycrystals
39. Anisotropic super-hardness of hexagonal WB2±z thin films10.1080/21663831.2021.2021308 ↗
40. Mechanical properties and phase stability of monoborides using density functional theory calculations
41. L. Lu, Y. Shen, X. Chen, L. Qian, K. Lu, Ultrahigh strength and high electrical conductivity in copper, 2004.10.1126/science.1092905 ↗
42. Strengthening and plasticity in nanotwinned metals10.1557/mrs.2016.60 ↗