In-situ synchrotron X-ray diffraction study of the precipitates-matrix interaction in a selective laser melted Al-Mg-Sc-Zr alloy
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Additive Manufacturing Materials and Processes · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. E. Starke Jr, J. Staley, Chapter 24: application of modern aluminum alloys to aircraft, in: Fundamentals of Aluminium Metallurgy: Production, Processing and Applications, 2011: pp. 747–783.10.1533/9780857090256.3.747 ↗
2. SLM-processed Sc-and Zr-modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
3. Microstructural features of Sc-and Zr-modified Al-Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
4. Criteria for developing castable, creep-resistant aluminum-based alloys–A review10.1515/ijmr-2006-0042 ↗
5. Microstructure and mechanical properties of selective laser melted Al-Zn-Mg-Si-Sc-Zr alloy with high hot-cracking resistance10.1016/j.jallcom.2023.172930 ↗
6. Microstructure, tensile properties and heat-resistant properties of selective laser melted AlMgScZr alloy under long-term aging treatment10.1016/j.msea.2021.142527 ↗
7. Coarsening-and creep resistance of precipitation-strengthened Al–Mg–Zr alloys processed by selective laser melting10.1016/j.actamat.2020.02.008 ↗
8. Mechanical behavior at elevated temperatures of an Al–Mn–Mg–Sc–Zr alloy manufactured by selective laser melting10.1016/j.msea.2021.142032 ↗
9. In-situ mechanical and microstructural characterization of miniaturized Al-Mg-Sc-Zr and AlSi10Mg specimens processed by laser powder-bed fusion (PBF-LB)10.1016/j.jmrt.2024.03.084 ↗
10. Effect of platform temperature on the porosity, microstructure and mechanical properties of an Al–Mg–Sc–Zr alloy fabricated by selective laser melting10.1016/j.msea.2018.06.049 ↗
11. Characterisation of a novel Sc and Zr modified Al–Mg alloy fabricated by selective laser melting10.1016/j.matlet.2017.03.089 ↗
12. Selective laser melting of a novel Sc and Zr modified Al-6.2 Mg alloy: processing, microstructure, and properties10.1016/j.powtec.2017.06.050 ↗
13. The modified Williamson-Hall plot and dislocation density evaluation from diffraction peaks10.1016/j.scriptamat.2022.114768 ↗
14. The convolutional multiple whole profile (CMWP) fitting method, a global optimization procedure for microstructure determination10.3390/cryst10070623 ↗
15. Crystallite size distribution and dislocation structure determined by diffraction profile analysis: principles and practical application to cubic and hexagonal crystals10.1107/S0021889801003715 ↗
16. Phases in rapidly cooled scandium-silicon samples10.1016/0925-8388(94)90744-7 ↗
17. Formation, microstructure, chemical long-range order, and stability of quasicrystals in Al–Pd–Mn alloys10.1557/JMR.1991.2646 ↗
18. Superior room-temperature ductility of typically brittle quasicrystals at small sizes10.1038/ncomms12261 ↗
19. Grain boundary misorientation dependence of β phase precipitation in an Al–Mg alloy10.1016/j.scriptamat.2014.01.003 ↗
20. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
21. Orientation dependent pinning of (sub) grains by dispersoids during recovery and recrystallization in an Al–Mn alloy10.1016/j.actamat.2023.118761 ↗
22. Recrystallization texture development in commercial Al-Mn-Mg alloys10.1016/1359-6454(95)00290-1 ↗
23. Revealing the atomistic nature of dislocation-precipitate interactions in Al-Cu alloys10.1016/j.jallcom.2019.05.110 ↗
24. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
25. Crystallographic orientation-dependent strain hardening in a precipitation-strengthened Al-Cu alloy10.1016/j.actamat.2020.116577 ↗
26. An analysis of the influence of the precipitate type on the mechanical behavior of Al - Cu alloys by means of micropillar compression tests10.1016/j.actamat.2020.05.040 ↗
27. Influence of the stress state on the cross-slip free energy barrier in Al: an atomistic investigation10.1016/j.actamat.2019.10.055 ↗
28. Strengthening mechanisms of an Al-Mg-Sc-Zr alloy10.1016/S1359-6454(02)00258-6 ↗
29. Coarsening resistance at 400 C of precipitation-strengthened Al–Zr–Sc–Er alloys10.1016/j.actamat.2011.07.057 ↗
30. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al (Sc) alloys10.1016/S1359-6454(02)00201-X ↗
31. The structure of ledges at plate-shaped precipitates10.1016/0001-6160(71)90145-3 ↗
32. 3-D morphology and growth mechanism of primary Al6Mn intermetallic compound in directionally solidified Al-3at.% Mn alloy10.1016/j.intermet.2011.12.015 ↗
33. Combining solution-, precipitation-and load-transfer strengthening in a cast Al-Ce-Mn-Sc-Zr alloy10.1016/j.actamat.2024.119683 ↗
34. Cast near-eutectic Al-12.5 wt.% Ce alloy with high coarsening and creep resistance10.1016/j.msea.2019.138440 ↗
35. Modeling the effect of Al3Sc precipitates on the yield stress and work hardening of an Al–Mg–Sc alloy10.1016/j.actamat.2007.12.039 ↗
36. Influence of Mn addition on the microstructure and mechanical properties of a directionally solidified γ-TiAl alloy10.1016/j.matchar.2018.01.029 ↗
37. Solute-induced strengthening during creep of an aged-hardened Al-Mn-Zr alloy10.1016/j.actamat.2021.117268 ↗
38. Natural aging behaviors of Al-Cu-Li alloy: PLC effect, properties and microstructure evolution10.1016/j.matchar.2021.111694 ↗
39. Impact of dispersoids’ distribution on portevin-le-chatelier effect and surface quality in Al–Mg-Sc-Zr alloys10.1016/j.msea.2023.145108 ↗