Synthesis of negative-thermal-expansion ZrW2O8 substrates

J.-C. Chen, G.-C. Huang, C. Hu, J.-P. Weng

Scripta Materialia· Volume 49· Issue 3
Publisher page

Abstract

Abstract A method for making ZrW 2 O 8 ceramic substrates is described. ZrW 2 O 8 ceramic substrates are formed by sintering for 6 h between 1155 and 1200 °C. The variation of the thermal expansion coefficient with the location and the mechanical properties can both be improved by the appropriate heat treatment. The thermal expansion coefficient, Young’s modulus, and apparent density increase at higher sintering temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Thermal Expansion and Ionic Conductivity · Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Graham · J. Am. Ceram. Soc. · 1959 · 42 · 57010.1111/j.1151-2916.1959.tb13575.x ↗
2. Chang · J. Am. Ceram. Soc. · 1967 · 50 · 21110.1111/j.1151-2916.1967.tb15084.x ↗
3. Martinek · J. Am. Ceram. Soc. · 1968 · 51 · 22710.1111/j.1151-2916.1968.tb11881.x ↗
4. Pryde · J. Phys. Condens. Matter · 1996 · 8 · 1097310.1088/0953-8984/8/50/023 ↗
5. Mary · Science · 1996 · 272 · 9010.1126/science.272.5258.90 ↗
6. Evans · Chem. Mater. · 1996 · 8 · 280910.1021/cm9602959 ↗
7. Sleight AW, Evans JSO, Mary TA. US Pat 5,514,360, 199610.1126/science.272.5258.90 ↗
8. Wilkinson · Am. Chem. Soc. · 1999 · 11 · 101
9. Kowach · J. Crystal Growth · 1999 · 212 · 16710.1016/S0022-0248(99)00892-1 ↗
10. Yamamura · Solid State Commun. · 2000 · 114 · 45310.1016/S0038-1098(00)00092-2 ↗
11. Fleming DA, Johnson DW, Kowach GR. US Pat 0031692, 200110.1063/1.1379984 ↗