High electrical resistivity of pressureless sintered in situ SiC–BN composites
Source abstract
Abstract
SiC–BN composites with a BN content of 6 wt.% were pressureless sintered to ∼99.4% theoretical density at 2200 °C for 1 h and found to have a high electrical resistivity of 1.24 × 1010 Ω cm. Starting B4C and C were added to react partially with Si3N4 for in situ synthesis of BN and also to serve as sintering aids. Interface diffusion of B and N from BN into SiC was crucial to improving the insulating and dielectric properties through carrier compensation without causing any obvious decrease in the thermal conductivity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Borrero-López · J. Am. Ceram. Soc. · 2007 · 90 · 54110.1111/j.1551-2916.2006.01421.x ↗
2. Lee · Scr. Mater. · 2005 · 52 · 15310.1016/j.scriptamat.2004.09.012 ↗
3. Kovalčíková · J. Eur. Ceram. Soc. · 2009 · 29 · 238710.1016/j.jeurceramsoc.2009.01.021 ↗
4. Charpentier · Scr. Mater. · 2009 · 60 · 48110.1016/j.scriptamat.2008.11.013 ↗
5. Steen · Ceram. Int. · 2000 · 26 · 84910.1016/S0272-8842(00)00027-4 ↗
6. She · J. Eur. Ceram. Soc. · 2004 · 24 · 33110.1016/S0955-2219(03)00225-5 ↗
7. Watari · J. Am. Ceram. Soc. · 2003 · 86 · 181210.1111/j.1151-2916.2003.tb03563.x ↗
8. Kinoshita · Acta Mater. · 1997 · 45 · 200110.1016/S1359-6454(96)00298-4 ↗
9. Zhang · Appl. Phys. Lett. · 2004 · 85 · 204710.1063/1.1794866 ↗
10. Nakano · J. Eur. Ceram. Soc. · 2004 · 24 · 368510.1016/j.jeurceramsoc.2003.12.019 ↗
11. Takeda · J. Am. Ceram. Soc. · 1987 · 70 · C26610.1111/j.1151-2916.1987.tb04895.x ↗
12. Can · J. Eur. Ceram. Soc. · 2007 · 27 · 136110.1016/j.jeurceramsoc.2006.05.053 ↗
13. Kim · J. Am. Ceram. Soc. · 2013 · 1
14. Zhan · J. Mater. Res. · 2002 · 17 · 232710.1557/JMR.2002.0341 ↗
15. Lipp · J. Eur. Ceram. Soc. · 1989 · 5 · 310.1016/0955-2219(89)90003-4 ↗
16. Ohba · Phys. Rev. B · 2001 · 63 · 11520710.1103/PhysRevB.63.115207 ↗
17. Kusunose · J. Am. Ceram. Soc. · 2002 · 85 · 268910.1111/j.1151-2916.2002.tb00515.x ↗
18. Zhang · J. Eur. Ceram. Soc. · 2002 · 22 · 255110.1016/S0955-2219(02)00115-2 ↗
19. Coblenz · J. Am. Ceram. Soc. · 1988 · 71 · 108010.1111/j.1151-2916.1988.tb05795.x ↗
20. Zheng · Mater. Sci. Eng. A · 2012 · 540 · 10210.1016/j.msea.2012.01.105 ↗
21. Kusunose · Nanotechnology · 2008 · 19 · 27560310.1088/0957-4484/19/27/275603 ↗
22. Zhang · Acta Mater. · 2001 · 49 · 7710.1016/S1359-6454(00)00297-4 ↗
23. Zhang · J. Am. Ceram. Soc. · 2001 · 84 · 147510.1111/j.1151-2916.2001.tb00863.x ↗
24. Zhang · J. Am. Ceram. Soc. · 2002 · 85 · 225610.1111/j.1151-2916.2002.tb00444.x ↗
25. Ruh · J. Am. Ceram. Soc. · 1984 · 67 · C8310.1111/j.1151-2916.1984.tb19518.x ↗
26. Yang · Mater. Chem. Phys. · 2008 · 107 · 47610.1016/j.matchemphys.2007.08.013 ↗
27. Tajima · J. Am. Ceram. Soc. · 1982 · 65 · C2710.1111/j.1151-2916.1982.tb10375.x ↗
28. Ikeda · Phys. Rev. B · 1980 · 22 · 284210.1103/PhysRevB.22.2842 ↗