journal article·2006-08

Precipitation induced densification in a sintered Al–Zn–Mg–Cu alloy

R.N. Lumley, G.B. Schaffer

Scripta Materialia· Volume 55· Issue 3
Publisher page

Abstract

It is demonstrated that slow cooling to 200 degrees C from a high sintering temperature (620 degrees C) reduces porosity in an Al-8Zn-2.5Mg-1Cu powder compact when compared to isothermal sintering at the higher temperature for a longer time. The reduction in porosity is attributed to shrinkage associated with removal of solute from the aluminium solid solution and heterogeneous precipitation of the eta phase (MgZn2), particularly onto pore surfaces. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Bauxite Residue and Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. German · 1985
2. Lenel · 1980
3. W.A. Kaysser, Liquid Phase Sintering, Powder Metallurgy – An Overview., The Institute of Metals Series on Powder Metallurgy, 1991, Institute of Metals, London, p. 183.
4. German · Metall. Trans. A · 1986 · 17A · 20510.1007/BF02643896 ↗
5. Danninger · Powder Metall. Int. · 1987 · 19 · 19
6. Lumley · Scripta Mater. · 1996 · 35 · 58910.1016/1359-6462(96)00195-9 ↗
7. Lumley · Scripta Mater. · 1998 · 39 · 108910.1016/S1359-6462(98)00278-4 ↗
8. N Lumley · Metall. Mater. Trans. A · 1999 · 30A · 168210.1007/s11661-999-0108-7 ↗
9. Polmear · 1995
10. Ber · Mater. Sci. Eng. A · 2000 · 280 · 9110.1016/S0921-5093(99)00661-9 ↗
11. Maloney · Scripta Mater. · 1999 · 41 · 103110.1016/S1359-6462(99)00253-5 ↗
12. J.B. Friauf, Ph.D thesis, California Institute of Technology, 1926.