journal article·2001-06

The effect of strain rate on the tensile deformation of Ti-6Al-4V/SiC composites

F. Gálvez, C. González, P. Poza, J. LLorca

Scripta Materialia· Volume 44· Issue 11
Publisher page

Abstract

Department of Materials Science. Polytechnic University of MadridE. T. S. de Ingenieros de Caminos. 28040 Madrid, Spain(Received November 2, 2000)(Accepted in revised form January 15, 2001)Keywords: Composites; Mechanical properties; Strain rate; FractureIntroductionThe search for lighter, stiffer and stronger materials has led to the reinforcement of light alloys withceramic fibers. In this respect, Ti alloys reinforced with SiC monofilaments stand out as the materialswith the best performance in term of specific stiffness and strength at intermediate temperatures (300°C to 700 °C). They were mainly aimed at gas turbine engines for aerospace vehicles, and significantprogress has been achieved over the last ten years, although their future is still dubious due to cost andother considerations (1–2). The effect of temperature and loading conditions (static or cyclic) on themechanical behavior of these composites has been extensively analyzed, but there is no informationavailable on their performance at high strain rates, so this investigation is focussed on this question.Apart from of its scientific interest, the response of fiber-reinforced Ti-alloy composites to thoseconditions is important from the practical viewpoint, as gas turbine components are often subjected tohigh strain rate and impact loading.Material and Experimental TechniquesThe composite material analyzed in this investigation was a Ti-6Al-4V alloy uniaxially reinforced with35 vol. % Sigma 11401 SiC fibers. Composite panels of 1.35 mm in thickness were manufactured byDERA (UK) by the foil-fiber-foil method. The panels were consolidated in vacuum at 940°C during 1hour under 30 MPa of pressure. The matrix filled completely the spaces between the fibers, whosecenters formed an imperfect hexagonal array. The Sigma 11401 fibers were processed by chemicalvapor deposition of b-SiC on a 15mm diameter tungsten wire, and a carbon coating of ’ 4 mm wasfinally deposited by the same method.Dog-bone specimens of 15 mm gage length and 3 mm width were machined with the fibers orientedin the loading direction using a water-jet. Tensile tests were carried out in a servo-hydraulic testingmachine with nominal cross-head speeds of 0.08 mm/min and 9 mm/min, which correspond to averagestrain rates of approximately 2 10
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Velocity Impact and Material Behavior · Fluid Dynamics Simulations and Interactions · Electromagnetic Launch and Propulsion Technology

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Larsen · Metall. Mater. Trans. · 1995 · 26A · 321110.1007/BF02669450 ↗
2. S. Mall and T. Nicholas, ed., Titanium Matrix Composites. Mechanical Behavior, Technomic, Lancaster, PA(1998).
3. Chocron · Int. J. Impact Eng. · 1997 · 19 · 13510.1016/S0734-743X(96)00017-6 ↗
4. J. A. Zukas, High Impact Dynamics, John Wiley & Sons, New York (1990).
5. Weber · Acta Metall. Mater. · 1994 · 42 · 344310.1016/0956-7151(94)90477-4 ↗
6. González · Adv. Comp. Lett. · 2000 · 9 · 295
7. Follansbee · Metall. Trans. · 1989 · 20A · 86310.1007/BF02651653 ↗
8. D. Ruiz, P. Hardy, and J. Harding, Report JH/000/1989, Solid Mechanics Group, Department of Engineering Science, University of Oxford (1989).
9. He · Acta Metall. Mater. · 1993 · 41 · 87110.1016/0956-7151(93)90021-J ↗
10. Landis · Int. J. Solids Struct. · 1999 · 44 · 433310.1016/S0020-7683(98)00193-0 ↗
11. C. González, Ph.D. thesis. Polytechnic University of Madrid (2000).