Abstract

Transparent conducting cadmium oxide (CdO) films have been deposited by spray pyrolysis. The film thicknesses have been determined using Rutherford backscattering spectrometry. X-ray diffraction measurements show that the films are polycrystalline with a preferential orientation along the (111) diffraction plane and the lattice parameter has been calculated. The dislocation density and strain have also been evaluated. The films possess a transmittance of about 75% in the visible and near-infrared region. The refractive index is found to vary between 1.68 and 2.84 in the wavelength range 500-1500 nm. The values of indirect and direct bandgaps obtained are 1.98 and 2.32 eV respectively. Hall effect measurements have been carried out in the temperature range 304-349 K. Resistivity, carrier concentration and mobility of the films at room temperature have been evaluated as 6.6*10-5 Omega m, 1.4*1025 m-3 and 0.68*10-2 m2 V-1 s-1 respectively. Thermoelectric power values from thermoelectric power measurements carried out in the temperature range 304-376 K have been found to be about 19.7-89 mu V K-1. Laser damage studies performed at a wavelength of 1.06 mu m indicate that the films possess a damage threshold density of about 2.37*104 J m-2.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: ZnO doping and properties · Chalcogenide Semiconductor Thin Films · Gas Sensing Nanomaterials and Sensors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Bädeker K · Ann. Phys., Lpz. · 1907 · 22 · 74910.1002/andp.19073270409 ↗
2. Balasundaram N · J. Mater. Sci. Lett. · 1994
3. Barret G · 1980 · 204
4. 10.1016/0038-1098(86)90920-810.1016/0038-1098(86)90920-8 ↗
5. Berry L G · 1967
6. Buerger M J · 1966 · 181
7. Chu T L · J. Electron. Mater. · 1990 · 19 · 100310.1007/BF02652928 ↗
8. Cullity B D · 1956 · 102
9. 10.1016/0040-6090(87)90320-810.1016/0040-6090(87)90320-8 ↗
10. Feldman L C · 1986 · 49
11. Finkenrath H · Z. Angew. Phys. · 1966 · 21 · 512
12. Gurumurugan K · Phys. Status Solidi · 1994 · 14310.1002/pssa.2211430111 ↗
13. 1961
14. Islam M N · J. Mater. Sci. Lett. · 1985 · 4 · 112510.1007/BF00720433 ↗
15. 10.1103/PhysRev.71.37410.1103/PhysRev.71.374 ↗
16. Lakshmanan T K · J. Electrochem. Soc. · 1963 · 110 · 54810.1149/1.2425811 ↗
17. Nelson J B · Proc. Phys. Soc. · 1945 · 57 · 16010.1088/0959-5309/57/3/302 ↗
18. Noguchi S · J. Phys. D: Appl. Phys. · 1980 · 13 · 112910.1088/0022-3727/13/6/023 ↗
19. Preston J S · Proc. R. Soc. · 1950 · 202A · 44910.1098/rspa.1950.0112 ↗
20. 10.1063/1.33703310.1063/1.337033 ↗
21. Sravani C · Semicond. Sci. Technol. · 1991 · 6 · 103610.1088/0268-1242/6/10/016 ↗
22. Tanaka K · Japan. J. Appl. Phys. · 1969 · 8 · 68110.1143/JJAP.8.681 ↗
23. Williamson G B · Phil. Mag. · 1956 · 1 · 3410.1080/14786435608238074 ↗