Electrical characteristics improvement of oxygen-annealed MOCVD-TiO2films
Source abstract
Abstract
As-grown and oxygen-annealed titanium oxide films grown on silicon substrate were studied. The titanium oxide films were prepared by metalorganic chemical vapour deposition in the temperature range of 400–650 °C. Compared with as-grown titanium oxide films, the oxygen-annealed titanium oxide films have better electrical properties and the stoichiometry of the titanium oxide film dominates the electrical properties. The leakage current can reach 2 × 10−7 A cm−2 under an applied field of 5 MV. The hysteresis loop shift voltage and interface state density are 6 mV and 2.6 × 1011 cm−2 eV−1, respectively.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · ZnO doping and properties · Advanced Memory and Neural Computing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. 10.1016/0040-6090(94)06445-810.1016/0040-6090(94)06445-8 ↗
2. 10.1116/1.57979210.1116/1.579792 ↗
3. Vydianathan K · J. Mater. Res. · 2001 · 16 · 183810.1557/JMR.2001.0253 ↗
4. Rausch N · Engineering · 1992 · 19 · 72510.1016/0167-9317(92)90531-U ↗
5. 10.1016/0038-1101(78)90308-810.1016/0038-1101(78)90308-8 ↗
6. 10.1016/0038-1101(62)90111-910.1016/0038-1101(62)90111-9 ↗
7. 10.1039/a802933d10.1039/a802933d ↗
8. 10.1016/S0169-4332(02)01228-X10.1016/S0169-4332(02)01228-X ↗
9. 10.1016/S0022-0248(01)01939-X10.1016/S0022-0248(01)01939-X ↗
10. 10.1063/1.11343010.1063/1.113430 ↗
11. 10.1149/1.183611810.1149/1.1836118 ↗
12. Sze S M · Physics of Semiconductor Devices · 1981
13. 10.1016/S0257-8972(00)00765-910.1016/S0257-8972(00)00765-9 ↗
14. 10.1063/1.35126410.1063/1.351264 ↗
15. Schroder D K · Semiconductor Material and Device Characterization · 1998 · 378
16. Nicollian E H · MOS (Metal Oxide Semiconductor) Physics and Technology · 1982
17. 10.1016/0038-1101(69)90065-310.1016/0038-1101(69)90065-3 ↗