Structure, morphology, optical and magnetic response of ZnO, Mn3O4and doped Zn0.5Mn0.5O nanoparticles as-synthesized using a chemical co-precipitation method
Source abstract
Abstract
Nano-polycrystalline samples of pristine and Mn-doped ZnO were synthesized using the feasible chemical co-precipitation method to investigate structural, vibrational and magnetic properties. From the x-ray diffraction pattern, ZnO was indexed and fitted in a single-phase wurtzite structure (hexagonal phase, P63mc). The simulation of Mn 3 O 4 was performed according to the initial parameter of tetragonal symmetry (I4 1 /amd space group). For the Zn 0.5 Mn 0.5 O sample, fitting was undertaken with both P6 3 mc and I4 1 /amd structural models, and showed that the diffraction profile is a result of the superposition of both spectral contributions. The average grain size obtained for different compositions of ZnO, Mn 3 O 4 , and Zn 0.5 Mn 0.5 O are 84.79, 72.26 and 68.24 nm, respectively. The optical band gap was obtained as 3.41 and 4.17 eV for the ZnO and Zn 0.5 Mn 0.5 O samples, respectively. The Raman spectrum of Zn 0.5 Mn 0.5 O also verified a mixed behaviour of ZnO and Mn 3 O 4 lattice vibration and presents two broad bands around 657 and 537 cm −1 . Room temperature magnetization–magnetic ( M – H ) field measurements showed the diamagnetic nature of ZnO, and the paramagnetic behaviour of Mn 3 O 4 , and Zn 0.5 Mn 0.5 O nanocrystalline samples.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: ZnO doping and properties · X-ray Diffraction in Crystallography · Copper-based nanomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References