Donor formation at 650 degrees C in oxygen-rich silicon after rapid thermal annealing of thermal donors
Source abstract
Abstract
Donor formation in oxygen-rich, n-type (100) silicon after rapid thermal annealing (RTA) of thermal donors (TDS) has been studied using resistivity measurements following annealing at 650 degrees C. The formation of so-called new donors (NDS) at 650 degrees C is enhanced by preannealing at 450 degrees C. However, ND formation occurs even in samples in which the complete annihilation of TDS has occurred by RTA at 800 degrees C. This suggests that some species generated during 450 degrees C preannealing, which are different from TDS, cause ND formation at 650 degrees C. The RTA behaviour of 450 degrees C preannealing-induced species shifts to the higher temperature by approximately 100 degrees C as compared with that of TDS. The behaviour of ND formation after RTA above 900 degrees C is consistent with that for as-grown samples without 450 degrees C preannealing.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (7)
Show source-provided references
1. Euller C S · J. Appl. Phys. · 1958 · 28 · 1546
2. 10.1063/1.32593610.1063/1.325936 ↗
3. 10.1063/1.9566510.1063/1.95665 ↗
4. 10.1063/1.33682010.1063/1.336820 ↗
5. Tokuda Y · J. Mater. Res. · 1989 · 4 · 24110.1557/JMR.1989.0241 ↗
6. 10.1063/1.34407610.1063/1.344076 ↗
7. 10.1016/0038-1101(68)90012-910.1016/0038-1101(68)90012-9 ↗