journal article·1991-05-01

Amorphous-crystalline transformation and conductivity enhancement in annealed bismuth sulphide thin films

P K Nair, J Campos, A Sanchez, L Banos, M T S Nair

Publisher page

Abstract

Post-deposition vacuum annealing of chemically deposited Bi2S3 thin films has been found to enhance the dark conductivity of the films from approximately=10-7 Omega cm-1 to approximately=102 Omega -1 cm-1 and the photoconductivity from approximately 10-5 Omega cm-1 to approximately=102 Omega cm-1. Such increase is attributed to (i) an amorphous-to-crystalline transformation of the setting in at approximately=175 degrees C, confirmed by X-ray diffraction studies and (ii) loss of sulphur from the film during vacuum annealing at temperatures >200 degrees C, confirmed by the absence of this effect in air/nitrogen annealing. In the case of annealing in air, the competing effect of mobility enhancement by amorphous-crystalline transformation and mobility depreciation by oxygen chemisorption at the intergrain region is seen to contribute to a dark conductivity and photoconductivity maxima at an annealing temperature of approximately=200 degrees C.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Transition Metal Oxide Nanomaterials · Thin-Film Transistor Technologies · Thermography and Photoacoustic Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Pramanik P · J. Electrochem. Soc. · 1980 · 127 · 208710.1149/1.2130072 ↗
2. Bhattacharya R N · J. Electrochem. Soc. · 1982 · 129 · 33210.1149/1.2123828 ↗
3. Biswas S · J. Electrochem. Soc. · 1986 · 133 · 4810.1149/1.2108539 ↗
4. Nair M T S · Semicond. Sci. Technol. · 1990 · 5 · 122510.1088/0268-1242/5/12/014 ↗
5. Nair P K · Semicond. Sci. Technol. · 1986 · 3 · 13410.1088/0268-1242/3/2/010 ↗
6. Savelli M · 1979 · 213
7. 10.1063/1.175488110.1063/1.1754881 ↗
8. 10.1063/1.33061810.1063/1.330618 ↗