Polyester/ether, poly (ethylene-1, 2-diphenoxyethane-p, p′-dicarboxylate) (PEET), fibers have been produced by high speed melt spinning method in the range of take-up velocity 500-7, 000m/min. Physical properties and structure of as-spun fibers were studied as a function of take-up speed and were compared with the drawn PEET fibers.Birefringence and density of the as-spun fibers largely increase with take-up speeds up to 3, 000m/min and then, their rates of increase slow down from this take-up speed onwards. Their take-up dependencies are not influenced by extrusion temperature. Good linear relationship is obtained between the logarithm of crystallinity (Xc) and birefringence (Δn). The intercept at Xc=100% gives Δn=0.280. This value agrees well with the intrinsic birefringence of the β form, 0.285.The fibers as-spun at above 3, 000m/min show a crystalline pattern of the β form on the equator and the higher order of (001) reflections are found on the meridian. The degree of crystalline orientation yields almost the perfect orientation from this take-up speeds onwards. During orientation crystallization in the spin-line, the crystal size is considerably developed in the direction perpendicular to the chain axis but not parallel to it with an increase in take-up speed. On the other hand, small angle x-ray long spacing increases with increase of take-up speed. This may be caused by the fact that a monomeric unit of PEET is large.Birefringence of the drawn fibers is not influenced neither with the drawing rate nor with the drawing temperature. Birefringence yields almost the same value if the draw ratio is the same despite the different drawing conditions. However, the fiber shows the different density and x-ray pattern.Birefringence and Young's modulus for the as-spun fibers give the equivalent values to those for the drawn fibers, however, the as-spun fibers show the β form and the drawn fibers show the α form. The maxima observed birefringence (Δn) and Young's modulus (E) combined with the intrinsic values (Δn∗=0.296, E∗=116 GPa for the α form and Δn∗=0.285, E∗=113 GPa for the β form) yield Δn/Δn∗=0.79, E/E∗=0.16 for the as-spun fibers and Δn/Δn∗=0.77, E/E∗=0.15 for the drawn fibers. These values are considerably higher than those for PET fibers obtained by high speed melt spinning method.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Polymer crystallization and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Tokyo Institute of Technology
Mitubishi Rayon Co.
References
Reference metadata was not supplied for this record.