WET SPINNING OF NYLON 3
Source abstract
Abstract
Nylon 3 was-spun in the ethyl acetate coagulation bath, using formic acid as the dope solvent. Spinning conditions, especially the drawing conditions were investigated.Boiling water, steam and glycerine, which are well-known drawing medias for ordinary polyamides were not suitable as the drawing media for nylon 3 fibers. While in such media as silicone oil, wood's metal or hot air, which are thought to have no interaction with polyamides, nylon 3 fibers were able to be stretched above the glass transition temperature (170_??_180°C). The drawn nylon fibers thus obtained showed fairly good mechanical properties as textile fibers, i. e. strength, 2_??_3g/d, elongation; 10_??_20%.Relations between mechanical properteis and spinning conditions were also investigated. Mechanical properties of drawn nylon 3 fibers thus obtained were not so much affected by coagulation conditions and spinning dope conditions, but remarkably affected by drawing conditions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fiber-reinforced polymer composites · Surface Modification and Superhydrophobicity · Material Properties and Processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Technical Research Laboratory, Asahi Chemical Industry Co., Ltd.
References
Reference metadata was not supplied for this record.