journal article·1955Open access

STUDIES ON THE RESIN FINISHING OF SILK-FABRICS

Akira Kuwahara

Sen'i Gakkaishi· Volume 11· Issue 7

Abstract

Studies on the relation of effects of the resin finishing on the crease-resistance of Silk-Habutae, performed by using the 5-section synthetic resins (Gelatin-cont. sec, Polyvinyl Acetate, Polymethyl Acrylate, Polyvinyliden chloride, Poly methyl Acrylate-Vinyl Acetate Co-polymer, and Methyrol melamine)(1) Methyrol melamine, Acrylate-Vinyl Acetate Co-polymer are more adhesive than other resins on 3rd section (1, 3 and 5%) at the resin adhesive volume.(2) On the crease-resistance, Gelatin, Polyvinyl Acetate and Methyrol melamine are prefered to other resins in the reversible angle of crease. When they are of higher concentration and the time of creasing is short hours of holding crease. In the long creasing however Polyvinyliden chloride, Acrylate-Vinyl Acetate Co-polymer and Polymethyl Acrylate are prefered to the former 3-resins.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silk-based biomaterials and applications · Dyeing and Modifying Textile Fibers · Textile materials and evaluations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.