THE STUDY ON WOOL PRESS FELTS
Source abstract
Abstract
Laps of parallel-laid webs were used as materials and hardened by the plate hardening machine. During this process the area of laps showed practically no change, but their breaking strength by g/tex unit remarkably increased. These facts may be due to an increase of inter-fiber bonds in the direction of thickness of laps.The plot of breaking strength vs. hardening time showed a sigmoidal-curve. This may be explained by a sharp increase of interlocking in an early stage of hardening process and a gradual increase of resistance for compression in the later stage.Lateral breaking strength of the hardened felt is always lower than longitudinal one, while the ratio of the both strengths increased from 0.25 to 0.55 by hardening. This increase of the strength ratio may be due to an increase of fiber orientation in the width direction of the hardened felts. A prolonged hardening of felt is undesirable from the point of view of the quality of products.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Mechanical stress and fatigue analysis · Metal Forming Simulation Techniques · Vibration and Dynamic Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Japan Felt Industrial Co., Ltd.
Department of Applied Chemistry, Konan University