Poly (ethylene terephthalate) fiber was continuously flow drawn with heating by CO2 laser irradiation. The flow drawing behavior was discussed with the view point of the irradiated laser energy and draw ratio. The drawing behavior can be classified into 4 categories ; (1) only stable neck drawing can be observed, (2) both neck and flow drawing can be observed, (3) only stable flow drawing can be observed, and (4) melt down or break. The fiber temperature and the fiber speed profile on the flow drawing process were measured. As the results, it revealed that the maximum fiber temperature on the drawing process was the range of 210 to 225 o C, and the length of deformation region increase with the draw ratio. The apparent elongational viscosity of the flow drawing process was also estimated by the measured fiber speed profiles, and was compared with the reported values of the neck drawing process and the meltspinning process. The minimum value of the apparent elongational viscosity was about 10 - 20 kPa·s regardless of the draw ratio.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Digital Media and Visual Art · Photopolymerization techniques and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Textile and Human Life Technology, Industrial Research Institute of Ishikawa,2-1, Kuratsuki, Kanazawa-shi, Ishikawa 920-8203, Japan
R&D Center, Huvis, Co., Ltd., 1690-1, Shinil-dong, Daedeok-gu, Daejeon-si, 306-230, Korea
Faculty of Textile Science and Technology, Shinshu University,3-15-1, Tokida, Ueda-shi, Nagano 386-8567, Japan
References
Reference metadata was not supplied for this record.