journal article·1956

PREPARATION OF POLYVINYLCHLORIDE FIBER

Tamio Yoshioka

Sen'i Gakkaishi· Volume 12· Issue 10
Publisher page

Abstract

Influences on the mechanical properties of the fiber by the fiber formation were studied to find the conditions of the industrial manufactures of the fiber which is prepared by spinning polyvinyl-chloride-tetrahydrofuran solution into water and the following results were obtained.(1) By change of spinning speed at the constant volume of exclusion, the change of denier accord with the theoretical value; tensile strength (g) shows nearly the constant value even if the denier is decreased, so, tensile strength (g/D) increases as the effect of decrease in denier, and elongation decreases in proportion to the draft between 2 and 4.(2) By change of the volume of exclusion, denier, tensile strengtn (g) and tenacity (g/D) show have almost the same results as by the change of the spinning speed but elongation shows the maximum at the draft 2.5.(3) At the constant draft adjusting the relations between the spinning speed and the volume of exclusion, denier, tensile strength (g) tenacity (g/D) and elongation show respectively the maximum at the spinning speed 25-30m/min. and 2.5 sec. of time passing through the congulation bath.(4) In the fixed condition of the heat-drawing process industrialy, high draft, spinning speed 20-25m/min. and the passing of more than 2.5 sec. through the coagulation bath are produce more satisfactory results; for the maximum drawing draft 2.5, spinning speed 25-30m/min. and 2.5 sec. in the coagulation bath are better.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Textile materials and evaluations · Electrospun Nanofibers in Biomedical Applications · Material Properties and Processing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.