Abstract

Carrotting conditions of the Angora rabbit guard hairs were studied by tracing the change in mechanical properties. The carrotting agents contained 1.8% of Hg(NO3)2 and 3.6% HNO3. The immersion was carried out at 20, 30, 45 and 60°C. The drying of the hairs after immersion was made for 2 days at room temperature or for 5, 15, 30, 60 and 120 mins. at 95°C respectively.As the results, it was observed that the mechanical properties of the hairs were modified remarkably by raising the immersion temperature but the effects of the drying temperature and time were negligibly small.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Textile materials and evaluations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Faculty of Technology, Tokyo Metropolitan University

References

Reference metadata was not supplied for this record.