Characteristics of plasmaless dry etching of silicon-related materials using chlorine trifluoride gas
Source abstract
Abstract
Silicon substrates and thermally grown oxide films were exposed to ClF 3 gas at various temperatures between room temperature and 600°C. Above room temperature, the activation energy of the silicon etch rate is 0.18 eV. The activation energy of SiO 2 etch rate below 400°C is estimated to be 0.12±0.01 eV. The obtained etch selectivity of silicon with respect to the SiO 2 is 100-300 between room temperature and 400°C. An enhanced etch rate is observed for the n-type silicon with low resistivity near room temperature. The ClF 3 gas, which has appropriate vapor pressure, has useful properties not only for in-situ cleaning but also for micromachining of silicon-related materials.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Plasma Diagnostics and Applications · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.