Design and Properties of New Lead-Free Solder Joints Using Sn-3.5Ag-Cu Solder
Source abstract
Abstract
This article aims to reduce the melting temperature of lead-free solder alloy and promote its mechanical properties. Eutectic tin-silver lead-free solder has a high melting temperature 221 ∘C used for electronic component soldering. This melting temperature, higher than that of lead–tin conventional eutectic solder, is about 183 ∘C. The effect of the melt spinning process and copper additions into eutectic Sn-Ag solder enhances the crystallite size to about 47.92 nm which leads to a decrease in the melting point to about 214.70 ∘C, where the reflow process for low heat-resistant components on print circuit boards needs lower melting point solder. The results showed the presence of intermetallic compound Ag3Sn formed in nano-scale at the Sn-3.5Ag alloy due to short time solidification. The presence of new intermetallic compound, IMC from Ag0.8Sn0.2 and Ag phase improves the mechanical properties, and then enhances the micro-creep resistance especially at Sn-3.5Ag-0.7Cu. The higher Young’s modulus of Sn-3.5Ag-0.5Cu alloy 55.356 GPa could be attributed to uniform distribution of eutectic phases. Disappearance of tin whiskers in most of the lead-free melt-spun alloys indicates reduction of the internal stresses. The stress exponent (n) values for all prepared alloys were from 4.6 to 5.9, this indicates to climb deformation mechanism. We recommend that the Sn95.7-Ag3.5-Cu0.7 alloy has suitable mechanical properties, low internal friction 0.069, low pasty range 21.7 ∘C and low melting point 214.70 ∘C suitable for step soldering applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Liew MC, Ahmad I, Lee LM et al (2012) Corrosion behavior of Sn-3.0Ag-0.5Cu lead-free solder in potassium hydroxide electrolyte. Metall Mater Trans A Phys Metall Mater Sci 43:3742–374710.1007/s11661-012-1194-5 ↗
2. Kamal M, El-Bediwi A, Lashin AR, El-Zarka AH (2011) Copper effects in mechanical properties of rapidly solidified Sn-Pb-Sb Babbitt bearing alloys. Mater Sci Eng A 530:327–33210.1016/j.msea.2011.09.092 ↗
3. Rosalbino F, Angelini E, Zanicchi G, Marazza R (2008) Corrosion behaviour assessment of lead-free Sn-Ag-M (M = In, Bi, Cu) solder alloys. Mater Chem Phys 109:386–39110.1016/j.matchemphys.2007.12.006 ↗
4. Zhang XP, Yu CB, Zhang YP et al (2007) Processing treatment of a lead-free Sn-Ag-Cu-Bi solder by rapid laser-beam reflowing and the creep property of its soldered connection. J Mater Process Technol 192–193:539–54210.1016/j.jmatprotec.2007.04.072 ↗
5. Suh D, Kim D, Liu P, Kim H (2007) Effects of Ag content on fracture resistance of Sn–Ag–Cu lead-free solders under high-strain rate conditions. Mater Sci Eng A 460:595–60310.1016/j.msea.2007.01.145 ↗
6. Shohji I, Yoshida T, Takahashi T, Hioki S (2004) Tensile properties of Sn–Ag based lead-free solders and strain rate sensitivity. Mater Sci Eng A 366:50–5510.1016/j.msea.2003.09.057 ↗
7. Sun L, Chen M, Zhang L, Yang F (2017) Microstructures evolution and properties of Sn-Ag-Cu solder joints. Acta Metall Sin 53:615–621
8. Mccormack M, Jin S (1994) Improved mechanical properties in new, Pb-free solder alloys. J Electron Mater 23:715–72010.1007/BF02651364 ↗
9. Meschter S, Snugovsky P, Bagheri Z et al (2014) Whisker formation on SAC305 soldered assemblies. JOM 66:2320–233310.1007/s11837-014-1183-9 ↗
10. Shohji I, Yasuda K, Takemoto T (2005) Estimation of thermal fatigue resistances of Sn-Ag and Sn-Ag-Cu lead-free solders using strain rate sensitivity index. Mater Trans 46(11):2329–233410.2320/matertrans.46.2329 ↗
11. Shalaby RM (2010) Effect of rapid solidification on mechanical properties of a lead free Sn-3.5Ag solder. J Alloys Compd 505:113–11710.1016/j.jallcom.2010.05.179 ↗
12. Williamson DM, Field JE, Palmer SJP, Siviour CR (2007) Rate dependent strengths of some solder joints. J Phys D Appl Phys 40:4691–470010.1088/0022-3727/40/15/051 ↗
13. Puttlitz KJ, Galyon GT (2007) Impact of the ROHS directive on high-performance electronic systems Part I: need for lead utilization in exempt systems. Lead-Free Electron Solder A Spec Issue J Mater Sci Mater Electron 40:331–346
14. Galyon GT (2005) Annotated tin whisker bibliography and anthology. IEEE Trans Electron Packag Manuf 28:94–12210.1109/TEPM.2005.847440 ↗
15. Shin SW, Yu J (2005) Creep deformation of Sn-3.5Ag-xCu and Sn-3.5Ag-xBi solder joints. J Electron Mater 34:188–19510.1007/s11664-005-0232-0 ↗
16. Pan HJ (2011) Synthesis of Sn-3.5Ag alloy nanosolder by chemical reduction method. Mater Sci Appl 2:1480–1484
17. Tsao LC (2011) Evolution of nano-Ag3Sn particle formation on Cu-Sn intermetallic compounds of Sn3.5Ag0.5Cu composite solder/Cu during soldering. J Alloys Compd 509:2326–233310.1016/j.jallcom.2010.11.010 ↗
18. Rosen G, Avissar J, Gefen Y, Baram J (1987) Centrifuge melt spinning. J Phys E 20:571–57410.1088/0022-3735/20/5/024 ↗
19. Kamal M, Mohammad U (2012) A review: chill-block melt spin technique, theories & applications ISBN: 978-1-60805-151-9, Bentham e Books, Bentham Science Publishers
20. Kamal M, Gouda E (2008) Effect of zinc additions on structure and properties of Sn–Ag eutectic lead-free solder alloy. J Mater Sci Mater Electron 19:81–8410.1007/s10854-007-9289-2 ↗
21. El-Bediwi A, Lashin AR, Mossa M, Kamal M (2011) Indentation creep and mechanical properties of quaternary Sn-Sb based alloys. Mater Sci Eng A 528:3568–357210.1016/j.msea.2011.01.054 ↗
22. Juhász A, Tasnádi P, Kovács I (1986) Superplastic indentation creep of lead—tin eutectic. J Mater Sci Lett 5:35–3610.1007/BF01671427 ↗
23. Roumina R, Raeisinia B, Mahmudi R (2004) Room temperature indentation creep of cast Pb-Sb alloys. Scr Mater 51:497–50210.1016/j.scriptamat.2004.05.048 ↗
24. Kamal M, El-Bediwi A, Jomaan M (2012) Rapid quenching of liquid lead base alloys for high performance storage battery applications, IJET-IJENS, 12, 06
25. Duwez P, Willens RH, Klement W (1960) Metastable electron compound in Ag-Ge alloys. J Appl Phys 31:113710.1063/1.1735778 ↗
26. Giessen BC, Grant NJ (1965) New intermediate phases in transition metal systems, III. Acta Crystallogr 18:1080–108110.1107/S0365110X65002566 ↗
27. Li JF, Agyakwa PA, Johnson CM (2012) Effect of trace Al on growth rates of intermetallic compound layers between Sn-based solders and Cu substrate. J Alloys Compd 545:70–7910.1016/j.jallcom.2012.08.023 ↗
28. Bieler TR, Jiang H (2006) Influence of Sn grain size and orientation on the thermomechanical response and reliability of Pb-free solder joints. IEEE Trans Compon Packag Technol 31(2):1462–1467
29. Cullity BD (1959) Elements of X-ray diffraction, vol 262. Addison-Wesley Publishing Company, USA, p 317
30. Kamal M, El-Bediwi A-B, Shalaby R, Younus M (2015) A study of eutectic indium-bismuth and indium-bismuth-tin Field’s metal rapidly solidified from melt. J Adv Phys 7:1404–141310.24297/jap.v7i2.1704 ↗
31. Van Arkel EA (1925) Über die Verformung des Kristallgitters von Metallen durch mechanische Bearbeitung. Physica 34:208–212
32. Williamson G, Hall W (1953) X-ray line broadening from filed aluminium and wolfram. Acta Metall 1:22–3110.1016/0001-6160(53)90006-6 ↗
33. Kamal M, El-Bediwi A-B (2000) Structure, mechanical metallurgy and electrical transport properties of rapidly solidified Pb50Sn50−xBix alloys. J Mater Sci Mater Electron 11(6):519–52310.1023/A:1008976820330 ↗
34. Shimoda M, Hidaka N, Watanabe H, Yoshiba M (2011) High temperature creep properties of Sn-3.5 Ag and Sn-5Sb lead-free solder alloys. Trans JWRI 40:2
35. Kumar R (2014) Effect of Ag on Sn-Cu lead free solders effect of Ag on Sn-Cu lead free solders. Thesis of PhD in Department of Metallurgical and Materials Engineering National Institute Of Technology, Rourkela
36. Shalaby RM (2013) Effect of silver and indium addition on mechanical properties and indentation creep behavior of rapidly solidified Bi-Sn based lead-free solder alloys. Mater Sci Eng A 560:86–9510.1016/j.msea.2012.09.038 ↗
37. Zu FQ, Zhu ZG, Zhang B et al (2001) Post-melting anomaly of Pb-Bi alloys observed by internal friction technique. J Phys Condens Matter 13:11435–1144210.1088/0953-8984/13/50/303 ↗
38. Sweatman K, Mcdonald SD, Whitewick M et al. (2013) Grain refinement for improved lead-free solder joint reliability. In: Proceedings of IPC APEX EXPO Conference & Exhibition 2013, APEX EXPO 2013, San Diego, United States, pp 561–589
39. Yi-Wen C, Thomas AS (2003) Predicting tensile properties of the bulk 96.5Sn-3.5Ag lead-free solder. J Electron Mater (32) 6(2003):1–19
40. Sun L, Zhang L (2015) Properties and microstructures of Sn-Ag-Cu-X lead-free solder. Adv Mater Sci Eng 2015:1–1610.1155/2015/639028 ↗
41. Pandher RS, Lewis BG, Vangaveti R, Singh B (2007) Drop shock reliability of lead-free alloys—effect of micro-additives. In: Proceedings - electronic components and technology conference, pp 669–67610.1109/ECTC.2007.373868 ↗
42. El-Ashram T, Shalaby RM (2005) Effect of rapid solidification and small additions of Zn and Bi on the structure and properties of Sn-Cu eutectic alloy. J Electron Mater 34:212–21510.1007/s11664-005-0234-y ↗
43. Kamal M, El-Ashram T (2007) Microcreep of rapidly solidified Sn–0.7 wt.% Cu–In solder alloys. Mater Sci Eng A 456:1–410.1016/j.msea.2007.01.056 ↗
44. Shalaby RM (2015) Indium, chromium and nickel-modified eutectic Sn–0.7 wt% Cu lead-free solder rapidly solidified from molten state. J Mater Sci Mater Electron 26:6625–663210.1007/s10854-015-3261-3 ↗
45. Lin C, Chu D (2005) Creep rupture of lead-free Sn-3. 5Ag and Sn-3. 5Ag-0. 5Cu solders. J Mater Sci Mater Electron 16:355–36510.1007/s10854-005-1147-5 ↗
46. Gumaan MS, Ali EA, Shalaby RM, Kamal M (2016) Improvement of the mechanical properties of Sn-Ag-Sb lead-free solders: effects of Sb addition and rapidly solidified. PCIM Eur 2016; Int Exhib Conf Power Electron Intell Motion, Renew Energy Energy Manag 9